نتایج جستجو برای: 316l steel

تعداد نتایج: 81785  

Journal: :international journal of iron & steel society of iran 2010
a. najafkhani k. zangeneh-madar h. abbaszadeh

in the present research, friction stir welding (fsw) process was used for butt joining of pure copper plate to 316l stainless steel plate. mechanical properties and microstructural characteristics of the joint were evaluated by microhardness and tensile tests as well as optical and scanning electron microscope (sem). it was found that microstructure of the weld nugget (wn) has fine grains where...

2016
Kazuhiro Imai Sachiko Hiromoto

Bulk metallic glasses (BMGs) show higher strength and lower Young's modulus than Ti-6Al-4V alloy and SUS 316L stainless steel. This study aimed to perform in vivo evaluations of Zr65Al7.5Ni10Cu17.5 BMGs for osteosynthesis devices. In the study for intramedullary implants, osteotomies of the femoral bones were performed in male Wistar rats and were stabilized with Zr65Al7.5Ni10Cu17.5 BMGs, Ti-6A...

Journal: :journal of modern processes in manufacturing and production 2013
mehdi arabbeigi mehran moradi boozarjomehr ghasemi majid sattar

one of the bellows producing method is hydroforming process .whereas some factor of hydroforming process specially internal pressure affects on final characteristics produced bellows such as bursting, wrinkling and wall thickness distribution. in this paper the effect of internal pressure factor in final quality of produced bellows will be investigated. in simulation of process, abaqus/explicit...

2016
DANIELA COVACIU ROMONTI INGRID MILOSEV IOANA DEMETRESCU

Dental alloys as CoCrMo, SS 316L stainless steel and NiTi were electrochemically investigated in artificial Fusayama saliva, unmodified and modified with two different concentrations of natrium fluoride. Electrochemical tests include measurements of open circuit, measurements of linear polarization, potentiodinamic polarization curves and electrochemical impedance spectra. The best electrochemi...

2017
Tao Wan Takashi Naoe Takashi Wakui Masatoshi Futakawa Hironari Obayashi Toshinobu Sasa

A lead bismuth eutectic (LBE) spallation target will be installed in the Target Test Facility (TEF-T) in the Japan Proton Accelerator Research Complex (J-PARC). The spallation target vessel filled with LBE is made of type 316L stainless steel. However, various damages, such as erosion/corrosion damage and liquid metal embrittlement caused by contact with flowing LBE at high temperature, and irr...

Journal: :Applied sciences 2022

Clad rebars of four different base materials (20MnSiV, 35# steel, 45# and 55# steel) were successfully produced by a vacuum hot rolling process. A metallographic optical microscope (OM), electron backscatter diffractometer (EBSD), probe micro-analyzer (EPMA), salt spray corrosion chamber used to investigate the clad contour, properties, composite interface microstructure all rebars. The results...

2005
H. S. Wang J. R. Yang H. K. D. H. Bhadeshia

The microstructure of 8 mm diameter wire produced by the severe deformation of 316L austenitic stainless steel has been examined using TEM and X-ray diffraction. The deformation imparted amounts to a true strain of 6.3. Data from previous studies on strain induced transformation of this steel have been combined with new results to show that true strains .2 are required in order to observe mecha...

Journal: :Acta of bioengineering and biomechanics 2009
Justyna Krzak-Roś Jarosław Filipiak Celina Pezowicz Agnieszka Baszczuk Mirosław Miller Maciej Kowalski Romuald Bedziński

Pure and calcium-doped silica and titanium dioxide thin films were prepared by the sol-gel method. Two different metallic substrates, i.e. stainless steel (316L) and titanium alloy (Ti6Al4V), were used for thin film deposition. Physicochemical properties and roughness of the thin films derived were investigated using the Raman spectroscopy, X-ray diffraction analysis, scanning electron microsco...

2016
Han-Seung Lee Jin-Ho Park Jitendra Kumar Singh Mohamed A. Ismail

Waste water treatment reservoirs are contaminated with many hazardous chemicals and acids. Reservoirs typically comprise concrete and reinforcement steel bars, and the main elements responsible for their deterioration are hazardous chemicals, acids, and ozone. Currently, a variety of techniques are being used to protect reservoirs from exposure to these elements. The most widely used techniques...

2003
M. Braic S. Zamfir M. Balaceanu V. Braic G. Pavelescu A. Zamfir A. Vladescu

The corrosion behavior of TiN coated 316L stainless steel in an artificial physiological solution was investigated by means of an electrochemical test. Two different PVD methods were used for film deposition: cathodic arc and reactive magnetron sputtering. The dependence of the corrosion resistance on the main deposition parameters (nitrogen pressure, substrate bias) was analyzed. For a better ...

نمودار تعداد نتایج جستجو در هر سال