Davood Rahmatabadi Enayatolah Mohemi Hesam Moghadasi Moslem Tayebi Ramin Hashemi,

In this paper, the reasons of damage water pumps parts of the air compressor cooling system were studied. To reach this goal, the works like preparing metallographic samples, evaluation of structure, investigation of mechanical properties, the alloy parts detection and chemical analysis of deposit and corrosion products collected from the parts were performed. According to studies and results o...

Journal: :Fatigue & Fracture of Engineering Materials & Structures 2002

Journal: :Journal of the Japan Institute of Metals and Materials 1974

2015
Liang Song Erjun Guo Liping Wang Dongrong Liu Hugo F. Lopez

The effects of silicon (Si) on the mechanical properties and fracture toughness of heavy-section ductile cast iron were investigated to develop material for spent-nuclear-fuel containers. Two castings with different Si contents of 1.78 wt.% and 2.74 wt.% were prepared. Four positions in the castings from the edge to the center, with different solidification cooling rates, were chosen for micros...

Davood Rahmatabadi Enayatolah Mohemi Hesam Moghadasi Moslem Tayebi Ramin Hashemi,

In this paper, the reasons of damage water pumps parts of the air compressor cooling system were studied. To reach this goal, the works like preparing metallographic samples, evaluation of structure, investigation of mechanical properties, the alloy parts detection and chemical analysis of deposit and corrosion products collected from the parts were performed. According to studies and results o...

2013
F. Iacoviello V. Di Cocco A. Rossi M. Cavallini

Ductile cast irons (DCIs) are characterized by a wide range of mechanical properties, mainly depending on microstructural factors, as matrix microstructure (characterized by phases volume fraction, grains size and grain distribution), graphite nodules (characterized by size, shape, density and distribution) and defects presence (e.g., porosity, inclusions, etc.). Versatility and higher performa...

2008
B. Stokes K. K. Lee P. A. S. Reed

Crack initiation and growth behaviour of an austempered ductile iron (ADI) austenitised at 800C and austempered at 260C has been assessed under three point bend fatigue conditions. Initiation sites have been identified as carbides remaining from the as cast ductile iron due to insufficient austenisation. The number of carbides cracking on loading to stresses greater than 275 MPa is critical in ...

A.R Kiani-Rashid, D. V. Edmonds

The influence of aluminium on the microstructure of austempered ductile cast iron (ADI) has been studied. A number of irons of different compositions have been made by green sand casting and gravity die casting of appropriate design to provide the experimental materials. Austenitising was carried out at different temperatures and holding times for a variety of experimental irons to achieve suff...