نتایج جستجو برای: آلیاژ تیتانیمti 6al 4v

تعداد نتایج: 6439  

2017
Mohammad Rizviul Kabir Henning Richter

A selective laser melting (SLM)-based, additively-manufactured Ti-6Al-4V alloy is prone to the accumulation of undesirable defects during layer-by-layer material build-up. Defects in the form of complex-shaped pores are one of the critical issues that need to be considered during the processing of this alloy. Depending on the process parameters, pores with concave or convex boundaries may occur...

Journal: :International journal of nanomedicine 2015
Elena Filova Jaroslav Fojt Marketa Kryslova Hynek Moravec Ludek Joska Lucie Bacakova

Ti-6Al-4V-based nanotubes were prepared on a Ti-6Al-4V surface by anodic oxidation on 10 V, 20 V, and 30 V samples. The 10 V, 20 V, and 30 V samples and a control smooth Ti-6Al-4V sample were evaluated in terms of their chemical composition, diameter distribution, and cellular response. The surfaces of the 10 V, 20 V, and 30 V samples consisted of nanotubes of a relatively wide range of diamete...

2015
Perumal Ganapathy Geetha Manivasagam Asokamani Rajamanickam Alagumurthi Natarajan

This paper presents the wear characteristics of the composite ceramic coating made with Al2O3-40wt%8YSZ on the biomedical grade Ti-6Al-4V alloy (grade 5) used for total joint prosthetic components, with the aim of improving their tribological behavior. The coatings were deposited using a plasma spraying technique, and optimization of plasma parameters was performed using response surface method...

Journal: :Journal of the Royal Society, Interface 2009
Chengtie Wu Yogambha Ramaswamy Xuanyong Liu Guocheng Wang Hala Zreiqat

Novel Ca-Si-Ti-based sphene (CaTiSiO5) ceramics possess excellent chemical stability and cytocompatibility. The aim of this study was to prepare sphene coating on titanium alloy (Ti-6Al-4V) for orthopaedic applications using the plasma spray method. The phase composition, surface and interface microstructure, coating thickness, surface roughness and bonding strength of the plasma-sprayed sphene...

در این پژوهش پوشش کربونیترید تیتانیم روی سطح آلیاژ Ti-6Al-4V به­روش نیتروژن-کربن­دهی نشانده شد و سازوکار جدایش پوشش از زیرلایه مورد بررسی قرار گرفت. به این ­منظور نمونه ­های مکعبی از آلیاژ مد­نظر درون محفظه حاوی گرافیت جاسازی شد و  مجموعه درون کوره تیوبی حاوی گاز نیتروژن قرار گرفت. پس از سنتز پوشش در دماهای1200 تا 1400 سانتی­گراد و زمان­ های 20، 40 و 60 دقیقه، بررسی­های ساختاری با استفاده از پر...

2016
W. Pawlak K. J. Kubiak B. G. Wendler T. G. Mathia

A significant improvement of tribological properties on Ti-6Al-4V has been achieved by developed in this study multilayer treatment method for the titanium alloys. This treatment consists of an intermediate 2 μm thick TiCxNy layer which has been deposited by the reactive arc evaporation onto a diffusion hardened material with interstitial O or N atoms by glow discharge plasma in the atmosphere ...

2017
Ming Yan Peng Yu

This chapter begins with an introduction of the fundamental properties of Ti-6Al-4V, and its densification mechanism, typical microstructure and mechanical property achievable by conventional PM routes. This functions as a point of reference for the following discussion of the AM Ti-6Al-4V in terms of densification, microstructure, and mechanical property. The mostly popular laser-based AM tech...

2016
Hansong Li Chuanping Gao Guoqian Wang Ningsong Qu Di Zhu

The titanium alloy Ti-6Al-4V is used in many industries including aviation, automobile manufacturing, and medical equipment, because of its low density, extraordinary corrosion resistance and high specific strength. Electrochemical machining (ECM) is a non-traditional machining method that allows applications to all kinds of metallic materials in regardless of their mechanical properties. It is...

2016
Kazuhiro Imai Sachiko Hiromoto

Bulk metallic glasses (BMGs) show higher strength and lower Young's modulus than Ti-6Al-4V alloy and SUS 316L stainless steel. This study aimed to perform in vivo evaluations of Zr65Al7.5Ni10Cu17.5 BMGs for osteosynthesis devices. In the study for intramedullary implants, osteotomies of the femoral bones were performed in male Wistar rats and were stabilized with Zr65Al7.5Ni10Cu17.5 BMGs, Ti-6A...

Sabet, H., Anbarzadeh, A. ,

The aim of this study is investigation of TLP variables on microstructure and mechanical properties of Al2024 to Ti-6Al-4V bonding for TLP joint. For this purpose, the sheets were prepared with dimension of 130×32×3 mm from Ti-6Al-4V and Al2024 alloys and 50µm thick Sn-5.3Ag-4.2Bi foil as interlayer. Sn-5.3Ag-4.2Bi foil prepared with dimension of 32×25 mm. Two alloys was joint together by proce...