نتایج جستجو برای: tailor welded blanks twbs gas tungsten arc welding
تعداد نتایج: 315905 فیلتر نتایج به سال:
In the present study, parameters of tool rotation speed, tool travel speed and tool offsetting with different levels were used in the friction stir welding (FSW) of aluminum-copper tailor welded blanks (TWBs). The FSW of pure copper to 5052 aluminum alloy were carried out by varying tool rotation speed from 800 rpm to 1200 rpm, tool travel speed from 40 mm/min to 80 mm/min and tool offsetting f...
Tungsten inert gas (TIG) welding, also called as gas tungsten welding 1. (a) Schematic of TIG welding Process (b) Variety of tungsten electrodes. The activated TIG (ATIG) welding process mainly focuses on increasing the depth of penetration and the reduction in the width of weld bead has not been paid. Tungsten inert gas welding, TIG is widely applied in manufacturing process for different The ...
An adaptive control based on fuzzy logic has been implemented for Gas Tungsten Arc Welding (GTAW). This adaptive controller eliminates the problems frequently experienced with traditional Automatic Voltage Control (AVC) systems, which do not adequately perform for all operational conditions because of the non-linear relationship between the arc voltage, current and arc length. This paper examin...
This paper presents the results of a study aimed at establishing the temperature distribution during the welding of magnesium alloy sheets by Pulsed Current Gas Tungsten Arc Welding (PCGTAW) and Constant Current Gas Tungsten Arc Welding (CCGTAW) processes. Pulsing of the GTAW welding current influences the dimensions and solidification rate of the fused zone, it also reduces the weld pool volum...
Currently there is a huge competition amongst the OEMs and manufacturers in the auto industry to reduce the weight of the car. A few design modifications or use of different size and grades of materials solves this problem greatly. This paper focuses upon the metal finishing process of Laser Welded Blanks (LWB) with simulation and reliability as well as new process development. These blanks are...
This paper aims at optimization of process parameters for gas tungsten arc welding (GTAW) of sheet samples of Aluminium alloy AA1100 using AC wave with Argon as inert gas. Tensile properties of parent and welded specimens were determined as per ASTM-E8M standard. Taguchi approach was applied to determine most influential control parameters which will yield better tensile strength of the joints ...
Cracking is a major concern in welding aluminum alloys. Although weld solidification cracks can be eliminated through the addition of filler metal, the additives modify the alloy or base metal constituents and may not always be desirable. High-energy beam processes, such as electron beam welding, that result in minimal heat input reduce crack sensitivity, but their high cost limits their applic...
In this study, microstructural features and mechanical properties of Incoloy 825-316L stainless steel dissimilar joints have been investigated. For this purpose, pulsed gas tungsten arc welding method was employed and 316L, Inconel 82 and Inconel 625 alloys were used as filler metal. First, specimens were cut. Pulsed gas tungsten arc welding was performed using peak and base currents of 220 A a...
In this study, microstructural features and mechanical properties of Incoloy 825-316L stainless steel dissimilar joints have been investigated. For this purpose, pulsed gas tungsten arc welding method was employed and 316L, Inconel 82 and Inconel 625 alloys were used as filler metal. First, specimens were cut. Pulsed gas tungsten arc welding was performed using peak and base currents of 220 A a...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید