نتایج جستجو برای: solvothermal method
تعداد نتایج: 1631216 فیلتر نتایج به سال:
cuins2 nanostructures were synthesized via a simple surfactant-free solvothermal route. in this synthesis, thiosemicarbazide and thioglycolic acid were used as sulfur sources. the effects of different parameters such as type of precursor and time on the morphology and particle size of the samples have been investigated. the nanostructures were characterized by means of ...
A general approach involving a solvothermal method was developed to synthesize a series of silicate nanoshells (<100 nm) where both Gd silicate and Gd silicate:Eu nanoshells were further demonstrated to exhibit dual-modality MRI and optical imaging functions.
A solvothermal method was developed for synthesizing organic monolayer protected amorphous calcium carbonate clusters using 10,12-pentacosadiynoic acid as ligand, ethanol as solvent and NaHCO3 decomposition as CO2 source, which can be extended to synthesize other monolayer protected mineral clusters.
The effect of temperature and water/thiourea ratio on the growth, crystallinity and morphological characteristics of CdS nanostructures synthetized by a solvothermal method using ethylenediamine as solvent were studied. The temperature and water/thiourea ratio used in the synthesis determine the surface area, shape, length and degree of crystallinity of the CdS nanostructures obtained. Nanowire...
Colloidal MoS(2) nanoparticles with diameters of less than 10 nm were prepared with a simple solvothermal method and demonstrated high efficiency in catalyzing H(2) evolution in Ru(bpy)(3)(2+)-based molecular systems under visible light.
A coordination polymer, [Co(II)(bIM)(acetate)] (bIM = benzimidazole) was synthesized using a solvothermal method; the complex has a two dimensional non-interpenetrated network structure and exhibits a spin-canted antiferromagnetic behaviour at low temperature and a high coercive field.
High quality MOF-5 crystals of 5-25 mum in size were prepared for the first time using a sonochemical method in substantially reduced synthesis time (ca. 30 min) compared with conventional solvothermal synthesis (24 h).
E-waste contains high amount of brominated flame retardants (BFRs) which are toxic, bioaccumulative and recalcitrant. In the present study, an effective and environmental-friendly process using solvothermal treatment to extract tetrabromobisphenol A (TBBPA), a typical BFR from waste computer housing plastic was developed. After the solvothermal process, TBBPA were transferred into a special sol...