نتایج جستجو برای: pitting corrosion resistance

تعداد نتایج: 401395  

2011
W. WALKE

The purpose of the tests was to determine whether and how sterilisation process of samples made of AISI 316L stainless steel with diff erent strain impacts their corrosion resistance. Tests were made on steel samples that had been electrochemically polished in order to assure proper surface roughness. In order to evaluate the infl uence of sterilisation on physical and chemical properties of st...

2014
Y. T. Zhou B. Zhang S. J. Zheng J. Wang X. Y. San X. L. Ma

Stainless steels are susceptible to the localized pitting corrosion that leads to a huge loss to our society. Studies in the past decades confirmed that the pitting events generally originate from the local dissolution in MnS inclusions which are more or less ubiquitous in stainless steels. Although a recent study indicated that endogenous MnCr2O4 nano-octahedra within the MnS medium give rise ...

M. Esfandiari, M. H. Moayed, M. Momeni,

Several surface modification techniques such as ion implantation, surface laser melting, have been employed to improve pitting corrosion resistance of stainless steel. Electropolishing is a technique in which the surface roughness is eliminated through a selective electrochemical dissolution. The effect of electropolishing on pitting corrosion of 304 stainless steel (SS) was investigated employ...

2012
N. Ramanaiah B. Balakrishna K. Prasad Rao

The corrosion behavior of the fusion zone of gas tungsten arc (GTA) welds of AA6061 alloy was studied. Role of gas tungsten arc welding techniques such as continuous current (CC) and pulsed current (PC) and reference filler (AA5356) were studied. Role of different grain refiners such as scandium, zirconium and Tibor in the reference filler was studied. Dynamic polarization testing was used to d...

2005

Allegheny Ludlum Type 316Ti (UNS S31635) is a titanium stabilized version of Type 316 molybdenum-bearing austenitic stainless steel. It is also known as DIN/EN designation No. 1.4571. The Type 316 alloys are more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels such as Type 304. They also offer higher creep, stress-ru...

2008
Mamdouh M. Salama

A mini-flowloop was developed to study CO2 corrosion and corrosion/erosion interactions, and to assess the effectiveness of inhibitors under conditions that simulate multi-phase pipelines. The miniflowloop was used to study the effect of testing time, steel chemistry, velocity, temperature, fluid chemistry, sand and inhibitors on corrosion rates. The measured corrosion rates in inhibited and un...

2003
Jan Olsson

The new superaustenitic stainless steel UNS S32654 (Avesta Sheffield 654 SMO) is proposed for condenser tubes in desalination and power plants. A number of tests illustrating its corrosion resistance in a variety of chloride containing environments are being reviewed in terms of pitting, crevice corrosion and stress corrosion cracking. Relevant mechanical and physical properties are described. ...

2005
K. Srinivasa K. Prasad

This review attempts to present the current understanding of the mechanism of pitting corrosion of heat treatable aluminium alloys and their welds. The role of alloying elements and intermetallic phases on the corrosion behavior of these alloys has been discussed. Pitting mechanism of aluminiumcopper alloys is specifically discussed. Finally effect of welding on the pitting corrosion of these a...

2015
Yu-Mei Han X.-Grant Chen

Aluminum based metal matrix composites (MMCs) have received considerable attention in the automotive, aerospace and nuclear industries. One of the main challenges using Al-based MMCs is the influence of the reinforcement particles on the corrosion resistance. In the present study, the corrosion behavior of Al-B₄C MMCs in a 3.5 wt.% NaCl solution were investigated using potentiodynamic polarizat...

2010
G. S. Frankel

Pitting corrosion is localized accelerated dissolution of metal that occurs as a result of a breakdown of the otherwise protective passive film on the metal surface. This paper provides an overview of the critical factors influencing the pitting corrosion of metals. The phenomenology of pitting corrosion is discussed, including the effects of alloy composition, environment, potential, and tempe...