Continuing our work on understanding the oxidation behavior of multiphase composite alloys based on the Mo-Si-B system, we investigated three alloys in the Mo-Si-B system, designated as A1, A2, and A3. The nominal phase assemblages of these alloys are: A1 = Mo5Si3Bx (T1)-MoSi2-MoB, A2 = T1Mo5SiB2 (T2)-Mo3Si, and A3 = Mo-T2-Mo3Si. Our previous work showed that for exposures to 1100°C, all alloys...
this study, MoSi2-TiB2 nanocomposites with 10 and 20 wt.% of TiB2 were synthesized by mechanical alloying through two different methods. In the first method, elemental powders of molybdenum, silicon, titanium and boron were milled together for 60 hours. In the second method, MoSi2 was made by 30-hours milling of Mo and Si. Then, commercial TiB2 was added to the matrix and milling was continued ...
Aluminium alloy composites have been extensively investigated for use in tribo-contact applications, however little detailed literature exists on the sub-surface microstructural evolution as a result of lubricated sliding wear. In this study two un-reinforced alloys (2124 & 5056) and identical alloy composites, reinforced with 15vol.% MoSi2 intermetallic particles were produced by a powder meta...
Like many other intermetallic materials, MoSi2 coatings are typically hard, but prone to catastrophic failure due to their low toughness at ambient temperature. In this paper, a self-assembled hierarchical structure that closely resembles that of nacre (i.e., mother of pearl) was developed in a MoSi2-based coating through a simple, yet cost-effective, depostion technique. The newly formed coati...
The cover illustrates the sintering of MoSi2/Al2O3/Feldspar heating elements fabricated by injection molding, thus allowing more complex geometries and economical element production, see article number 2100517 Dirk Penner co-workers. Different binder systems are investigated various shapes as shown in illustration produced tested. (Cover design: René Wick-Joliat)
To prevent premature triggering of the healing reaction in Mo-Si containing self-healing thermal barrier coating system, an oxygen impenetrable shell (α-Al2O3) around sacrificial particles (MoSi2) is desired. Here encapsulation method presented through selective oxidation Al Mo(AlxSi1-x)2 particles. Healing designed terms alumina thickness, particle size and fraction dissolved. By replacing Si ...
در این تحقیق ابتدا پودرهای mosi2 و mo(si,al)2 با استفاده از روش سنتز احتراقی دمابالای خود گستر (shs) سنتز شدند. نتایج بدست آمده از آنالیز xrd پودرهای حاصله نشان از سنتز قابل قبول این دو ترکیب با استفاده از این روش دارد. بدلیل وجود ناخالصی اکسیژن در محیط و در نمونه قبل از سنتز، نمونه های mosi2 ،دارای مقدار کمی فاز ناخالصی sio2 آمورف و نمونه های mo(si,al)2 دارای فاز ناخالصی بلوری al2o3 شدند. پس ا...
In this study, the oxidation stability up to 1000 °C in air of Hf(C,N)-MoSi2 composites was explored under non-isothermal and isothermal conditions. Composites with 1, 5, 10, 20% volume fractions were produced by low-energy ball milling subsequent spark plasma sintering. Differential scanning calorimetry (DSC) thermogravimetric (TG) coupled mass spectrometry used reveal staging process dependin...