Abstract: The effect of phase development on peel strength of alumina-copper metalized joint has been investigated. The alumina-copper joint was prepared in three stages. The alumina substrate was, first, metalized at 1500°C in H2-furnace by a new formulation. In the second step, a nickel layer was electroplated on the metalized layer with approximately 10µm thickness. Finally, copper strip...
objective (s):rheumatoid arthritis (ra) is a chronic systemic inflammatory disorder, primarily targeting the synovium and articular cartilage that leads to joint damage. recent reports have suggested the role of adipocytokines in mediating joint damage; however it still is a matter of debate. the purpose of this study was to evaluate the association between serum values of adiopocytokines (lept...
Transient liquid phase (TLP) bonding of AISI 304L stainless steel was carried out using BNi-2 amorphous interlayer. The microstructure of the joint area was studied by using optical and scanning electron microscopes and energy dispersive spectroscopy. The effect of bonding temperature (1030-1110 °C) was studied on the microstructure and corrosion behavior of the TLP bonded samples. Electrochemi...
Transient liquid phase (TLP) bonding of AISI 304L stainless steel was carried out using BNi-2 amorphous interlayer. The microstructure of the joint area was studied by using optical and scanning electron microscopes and energy dispersive spectroscopy. The effect of bonding temperature (1030-1110 °C) was studied on the microstructure and corrosion behavior of the TLP bonded samples. Electrochemi...
The aim of this study is investigation of TLP variables on microstructure and mechanical properties of Al2024 to Ti-6Al-4V bonding for TLP joint. For this purpose, the sheets were prepared with dimension of 130×32×3 mm from Ti-6Al-4V and Al2024 alloys and 50µm thick Sn-5.3Ag-4.2Bi foil as interlayer. Sn-5.3Ag-4.2Bi foil prepared with dimension of 32×25 mm. Two alloys was joint together by proce...
The aim of this study is investigation of TLP variables on microstructure and mechanical properties of Al2024 to Ti-6Al-4V bonding for TLP joint. For this purpose, the sheets were prepared with dimension of 130×32×3 mm from Ti-6Al-4V and Al2024 alloys and 50µm thick Sn-5.3Ag-4.2Bi foil as interlayer. Sn-5.3Ag-4.2Bi foil prepared with dimension of 32×25 mm. Two alloys was joint together by proce...
In this study, to bond AA2024 and AA6061 alloys to each other, three elements (Sn, Zn and Ga) were considered as interlayer elements in terms of atomic diffusion depth in the base metal and storage at 453°C for 2 days, 10 hours, 210 minutes, and 30 seconds that they were examined for atomic diffusion modeling. Finally, the two alloys were connected at a temperature of 453°C in a furnace enviro...
In this study, to bond AA2024 and AA6061 alloys to each other, three elements (Sn, Zn and Ga) were considered as interlayer elements in terms of atomic diffusion depth in the base metal and storage at 453°C for 2 days, 10 hours, 210 minutes, and 30 seconds that they were examined for atomic diffusion modeling. Finally, the two alloys were connected at a temperature of 453°C in a furnace enviro...