نتایج جستجو برای: coke amount
تعداد نتایج: 256248 فیلتر نتایج به سال:
In order to utilize high sulfur (3-6%) coals in various industries which otherwise cannot be utilized directly or even as a blend, studies on pyrolysis of four high sulfur NE regions Indian coals viz. 60ft Tikak, 20ft Tikak, Surupi and Bapung coal from Makum Coalfields of Meghalaya in presence of hydrogen were carried out at 900C. The steam was generated by heating waste water followed by its s...
Conversion of propanal to gasoline-range molecules was investigated over a series of HZSM-5 catalysts with controlled mesoporosity generated by desilication. Characterization of the structure of the solid by powder X-ray diffraction (XRD), scanning electronic microscopy (SEM), ammonia and isopropylamine temperature programmed desorption (TPD), and n-butane diffusivity measurements confirmed the...
Nano-SAPO-34 molecular sieves synthesized in a microwave environment with 20 nm crystal size showed a longer lifetime than SAPO-34 prepared by the conventional hydrothermal method in the reaction of methanol to olefins. It has been found that silicon distribution strongly affects the lifetime and selectivity. Thus, silicon at the border of the silicon islands gives a higher lifetime and lower C...
Quantitative analysis by X-ray powder diffraction of two cokes (pitch coke and petroleum coke) shows that their crystal structure changed with increasing temperature. The crystal data processing of the crystallization degree of disorder is used with further improvement of the proposed microcrystalline-stacking fault calculation method. With this improvement it is now possible to obtain the degr...
Accumulating evidence has shown that both DNA damage caused by the metabolites of polycyclic aromatic hydrocarbons (PAH) and genetic polymorphisms in PAH-metabolic genes contribute to individual susceptibility to PAH-induced carcinogenesis. However, the functional relevance of genetic polymorphisms in PAH-metabolic genes in exposed individuals is still unclear. In this study of 240 coke-oven wo...
The presence of pyrolytic carbon deposits can cause a number of serious problems in the operation of a coke oven. They can inhibit the flow of gas out of the oven; their removal may cause damage to the refractories and the coke pusher equipment, in particular when the deposition is extensive, and can affect the sealing of the oven so leading to undesirable emissions. Some plants burn off the ca...
Abstract. In order to keep stable in reinforcement learning process, a novel robust reinforcement learning decoupling control (RRLDC) based on integral quadratic constraints(IQC)is presented in this paper. It composes of a linear model to approximate the nonlinear plant, a state feedback K controller to generate the basic control law, and an adaptive critic unit to evaluate decoupling performan...
A novel utilization method of filter residue from the preparation process of zeolite-based catalysts was investigated. Y zeolite and a fluid catalytic cracking (FCC) catalyst were synthesized from filter residue. Compared to the Y zeolite synthesized by the conventional method, the Y zeolite synthesized from filter residue exhibited better thermal stability. The catalyst possessed wide-pore dis...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید