نتایج جستجو برای: aisi h13 hot work tool steel
تعداد نتایج: 1405385 فیلتر نتایج به سال:
Welding hot-work tool steels, containing 0.3-0.6% of carbon, is difficult both because of the elevated carbon content and because of significant hardening resulted from large amounts of alloying elements. A development of welding technology, i.e. better quality of electrodes, modern welding devices, improved welding technologies and better steel quality, make welding of such steel types possibl...
Electron BackScatter Diffraction (EBSD) in conjunction with Field-Emission Environmental Scanning Electron Microscopy (FEG-ESEM) has been used to evaluate the microstructural and local plastic strain evolution in different alloys (AISI 1005, AISI 304L and Duplex 2205) deformed by a single-stage cold and warm forging process. The present work is aimed to describe the different behavior of the au...
This paper presents the suitable depth of cut, spindle speed and feed rate that will be chosen during machining. If thus parameters are not considered, this can provoke abnormal tool behavior such as chatter. Chatter will limit the tool life which only can be use for just a few times. To predict the chatter occurs, the parameters will be use are spindle speed, depth of cut and feed rate. CNC ma...
The influence of the deformation grade on the recrystallised grain size has been studied in the AISI 304 stainless steel. Therefore, cold rolled samples of this material with reductions varying between 30% and 80% were annealed at different temperatures and subsequently quenched. The mean austenitic grain sizes were measured and compared. Moreover, the correlation between the variation of the t...
Laser powder bed fusion is an attractive manufacturing technology promising novel components for the aircraft, automobile, and medical industries. However, depending on material, some defects in parts, especially pores or microcracks, cannot be avoided LPBF process. To achieve a part with low defect density, optimal parameter sets must determined. Many investigations have focused how laser spee...
Complex two-component peak of anelastic mechanical losses was observed in multicomponent substitutional austenitic alloys after prior plastic deformation. In AISI 316L, AISI 316LN, AISI 310 and AISI 304 austenitic stainless steels, this peak is situated in the wide range of temperature from 200 to 400K. Characteristics of the observed peak for different thermo-mechanical treatments were studied...
INTRODUCTION Contaminated sponges might lead to cross-contamination in kitchens since they can transfer microorganisms to surfaces where microorganisms can survive for hours or days and contaminate food. The main objective of this study was to evaluate the transfer and the survival of bacteria from kitchen sponges to surfaces of AISI 316 stainless steel and polyethylene. METHODOLOGY Twenty-fo...
behaviors of stress corrosion cracking (scc)in martensitic stainless steel(aisi 420) and low carbon austenitic stainless steel (aisi 316l) have been compared under different conditions of temperature, environment (mgcl2), and strain rate. the results show that decreasing strain rate has detrimental effect on mechanical properties of both steels, including their strength and ductility. fractogra...