in this work, dynamic mechanical properties of three high-manganese steels with trip/twip or fully twip characteristics are studied. high strain rate experiments in the range of true strain rates between ~500 and 1800 /s are conducted using a dynamic torsional testing setup. all the three steels show a positive strain rate sensitivity in the intermediate range of strain rates (up to 500 /s). bu...
Metal additive manufacturing has strongly gained scientific and industrial importance during the last decades due to the geometrical flexibility and increased reliability of parts, as well as reduced equipment costs. Within the field of metal additive manufacturing methods, selective laser melting (SLM) is an eligible technique for the production of fully dense bulk material with complex geomet...
Low stacking fault energy face centered cubic (FCC) materials contain characteristic defect structures. Stacking fault tetrahedral are one of those rare structures that occur under special experimental conditions. For the first time, stacking fault tetrahedral were observed in Fe-30Mn-3Al-3Si twinning induced plasticity (TWIP) steel. Their presence resulted from a quenching heat treatment.
in this study, the effect of tensile test temperature (148 to 673 k) on the microstructural evolutions and the mechanicalproperties of high manganese twinning induced plasticity (twip) steel with the chemical composition of fe-31mn-3al-3si (wt. %) was investigated. xrd, sem and tem were used to study the microstructural evolutions.stacking fault energy (sfe) of the alloy was also calculated by ...
In this work, dynamic mechanical properties of three high-manganese steels with TRIP/TWIP or fully TWIP characteristics are studied. High strain rate experiments in the range of true strain rates between ~500 and 1800 /s are conducted using a dynamic torsional testing setup. All the three steels show a positive strain rate sensitivity in the intermediate range of strain rates (up to 500 /s). Bu...
low stacking fault energy face centered cubic (fcc) materials contain characteristic defect structures. stackingfault tetrahedral are one of those rare structures that occur under special experimental conditions. for the first time,stacking fault tetrahedral were observed in fe-30mn-3al-3si twinning induced plasticity (twip) steel. theirpresence resulted from a quenching heat treatment.
To meet the demand of 10% weight reduction goal for automotive steel, microstructure and mechanical properties Fe-18Mn-Al-C steel with different carbon aluminum contents were investigated under solid solution treatments, deformation mechanisms experimental steels elucidated. Aided by thermodynamic calculation, transmission electron microscopy (TEM) in situ scanning microscope (SEM) analysis, it...
The microstructures, mechanical properties, and anticorrosion properties of Fe–25Mn–Cr(12, 18 wt.%)–CN TWIP steels compared with nominal Fe–22Mn–0.6C steel (TWIP-ref) in the solid-solution state were investigated present study by using X-ray diffraction (XRD), electron backscattered (EBSD), transmission microscopy (TEM), tensile tests, potentiodynamic polarization measurement, etc. results show...
The quantitative characterization of the microstructure evolution in high-Mn steel during deformation is of great importance to understanding its strain-hardening behavior. In the current study, in situ high-energy synchrotron X-ray diffraction was employed to characterize the microstructure evolution in a Fe-17Mn-1.5Al-0.3C steel during a tensile test. The microstructure at different engineeri...