Copper smelting slags are hard materials. Therefore,to recover their copper by flotation method, grinding should be carried out to obtain optimal particle size. Copper smelting slags in the Bardeskan district, with work index of 16.24 kwh/st, were grinded for 65 minutes to reach an acceptable degree of freedom for the flotation tests, with particle size of 80%, smaller than 70 μm. With this gri...

Journal: :iranian journal of chemistry and chemical engineering (ijcce) 2005
ramdane salhi

the main aim of this research is to determine optimal leaching conditions; eh, ph and complexing agent concentrations, for recovery of copper from hydroxide sludges such as those produced by electroplating shops, metal finishers, treatment of acid mine drainage, and industrial wastewater in general. this has been preceded by a theoretical approach and numerical and computer calculation. potenti...

Journal: :analytical and bioanalytical chemistry research 0
zahra kaboli tanha university of zanjan, zanjan, iran mahdieh koorepazan moftakhar university of zanjan, zanjan, iran mohammad reza yaftian university of zanjan, zanjan, iran nader noshiranzadeh university of zanjan, zanjan, iran

oxime extractants 3-tert-butyl-2-hydroxy-5-methyl benzaldehyde oxime (hl1) and 3-tert-butyl-2-hydroxy-5-methoxy benzaldehyde oxime (hl2) were synthesized and characterized by conventional spectroscopic methods. suitable lipophilic nature of the prepared extractants allowed examining the ability of these molecules for extraction-separation of copper from its mixture with normally associated meta...

پایان نامه :وزارت علوم، تحقیقات و فناوری - دانشگاه شهید باهنر کرمان - دانشکده فنی 1392

معدن مس دره زار در استان کرمان،80 کیلومتری شمال شرق سیرجان، 19 کیلومتری شرق بخش پاریز، در فاصله 10 تا 12 کیلومتری جنوب معدن مس سرچشمه قرار دارد. این معدن دارای ذخیره 282 میلیون تن با عیار 38/0 درصد مس با کالکوپیریت بعنوان کانی اصلی مس می باشد که 88 درصد ذخیره آن مربوط به زون هایپوژن و 12 درصد مربوط به زون سوپرژن است. در این تحقیق با تهیه نمونه نماینده از سنگ معدن مس دره زار و انجام مطالعات کا...

The new copper processing plant of the Sarcheshmeh copper complex consists of two parallel circuits. After a primary crushing, the ore is sent to a SAG mill, and the product is further ground in a ball mill. The overflow of the hydrocyclones is fed to a flotation circuit that contains 8 rougher tank cells (RCS130), 3 cleaner cells (RCS50), 5 scavenger cells (RCS50), and a flotation column (as r...

In this work, the parameters affecting the recovery of copper from the low-grade sulfide minerals of Sarcheshmeh Copper Mine were studied. A low-grade sulfide ore was used with a copper grade of 0.25%, which was about 28% of the mineral oxide, and the sulfide minerals made up the rest. Much more sulfide minerals were found to be pyrite and most of the gangue minerals were quartz, anorthite, bio...

Texture and color appearance of froth is a discreet qualitative tool for evaluating the performance of flotation process. The structure of a froth developed on the flotation cell has a significant effect on the grade and recovery of copper concentrate. In this work, image analysis and neural networks have been implemented to model and control the performance of such a system. The result reveals...

However, the conventional gold recovery process is cyanidation, due to the recent environmental laws; researchers are looking for alternative methods for the recovery of gold. Furthermore, the copper anode slime is one of the most important secondary sources of gold (about 1200 ppm). So, the main objective of the current work is gold separation from copper anode slime as a rich secondary source...

Although bioleaching of chalcopyrite by thermophilic microorganisms enhances the rate of copper recovery, a high temperature accelerates iron precipitation as jarosite, which can bring many operational problems in the industrial processes. In this research work, the bioleaching of chalcopyrite concentrate by the thermophilic Acidianus brierleyi was studied, and the microbial grow...

The main aim of this research is to determine optimal leaching conditions; Eh, pH and complexing agent concentrations, for recovery of Copper from hydroxide sludges such as those produced by electroplating shops, metal finishers, treatment of acid mine drainage, and industrial wastewater in general. This has been preceded by a theoretical approach and numerical and computer calculation. Pot...