We propose an image-based framework to evaluate the uncertainty in the estimation of the volume fraction of specific microstructures based on the observation of a single section. These microstructures consist of cubes organized on a cubic mesh, such as monocrystalline nickel base superalloys. The framework is twofold: a model-based stereological analysis allows relating two-dimensional image ob...
Nickel-based superalloys have excellent properties at high temperatures, which makes them appropriate for applications such as turbocharges and aeronautic gas turbines. MAR-M246 is a superalloy developed these kinds of applications. The objective this work was to study the total replacement Ta by Nb in atomic percentage superalloy, regarding oxidation resistance. Although both elements same rol...
Decades of research has been focused on improving the high-temperature properties of nickel-based superalloys, an essential class of materials used in the hot section of jet turbine engines, allowing increased engine efficiency and reduced CO2 emissions. Here we introduce a new 'phase-transformation strengthening' mechanism that resists high-temperature creep deformation in nickel-based superal...
Abstract: The investigation is carried out to characterize welding of AISI 310 austenitic stainless steel to Inconel 657 nickel-chromium superalloy. The welds were produced using four types of filler materials: the nickel-based corresponding to Inconel 82, Inconel A, Inconel 617 and austenitic stainless steel 310. This paper describes the effects of aging treatment on the joint. The compara...
Laser cladding is a well-established process to apply coatings on metals. However, on substrates considerably thinner than 1 mm it is only rarely described in the literature. In this work 200 µm thin sheets of nickel-based superalloy 718 are coated with a powder of a cobalt-based alloy, Co-28Cr-9W-1.5Si, by laser cladding. The process window is very narrow, therefore, a precisely controlled Yb ...
Rene-80 nickel-base superalloy as an alloy for production of the jet turbine blades shows high mechanical properties as well as microstructure stability during the high temperature engine operation. In this research, age hardening heat treatment cycle was done on the as-cast Rene-80 superalloy. In the following, microstructure, elemental analysis of phases and macro-hardness of the alloy before...
Fatigue crack growth was investigated in Haynes 230, a nickel-based superalloy. Anisotropic stress intensity factors were calculated with a least squares algorithm using the displacements obtained from digital image correlation. Crack opening/sliding levels were measured by analysing the relative displacement of crack flanks. Reversed crack tip plastic zones were calculated adopting an anisotro...