نتایج جستجو برای: ips emax press
تعداد نتایج: 76834 فیلتر نتایج به سال:
Introduction: To achieve acceptable clinical performance, a ceramic veneer must be bonded to enamel by well-polymerized resin cement. Among different factors, thickness and translucency of the ceramic may affect the resin cement polymerization. Thus, the current study evaluated the effect of the thickness and translucency of lithium disilicate ceramic on light-cured resin cement bond strength t...
Background and Aims: The purpose of this in vitro study was to assess the effect of two different surface treatments on the contrast ratio of IPS e.max press ceramic submitted to accelerated aging. Materials and Methods: Ten ceramic (IPS e.max Press) disks (10-mm diameter and 1.5-mm thick) were fabricated according to the manufacturer's recommendations. The samples were randomly divided into 2...
خلاصه: سابقه وهدف: با توجه به اهمیت میزان پلیمریزاسیون سمان های رزینی بر طول عمر ترمیم های غیر مستقیم و خلا اطلاعاتی موجود در این زمینه این تحقیق به هدف تعیین تاثیر ضخامت های مختلف پرسلن IPS e.max Press بر میزان پلیمریزاسیون سمان رزینی Light cured Choice 2 با روش FTIR در واحد دندانپزشکی دانشگاه آزاد اسلامی تهران در سال 1393 انجام شد. مواد و روش ها: در این تحقیق Experimental از نوع (in vitro) 4...
Objectives: The effect of ceramics construction (pressable, machinable) and corrosion on flexural strength and micro-hardness was studied. Materials & Methods: Two types of ceramics were tested: IPS e-max Press and IPS e-max CAD. Forty samples were constructed and divided into 2 groups according to the type of ceramics. Each group was then subdivided into 2 subgroups. Subgroups 1 were not subje...
مقدمه: یکی از مشکلات روکشهای تمام سرامیکی، امکان شکستن آنها در برابر نیروهای اکلوزالی است. هدف از این تحقیق مقایسه مقاومت به شکست روکشهای تمام سرامیکی IPS e.max در دو ختم تراش چمفر و شولدر بود. مواد وروشها: برای انجام این مطالعه آزمایشگاهی، بر روی یک دندان پرمولار اول ماگزیلا مارژین چمفر ˚50 (8/0 میلیمتر) تراشیده شد و 20 بار توسط پلی وینیل سایلوکسان قالبگیری شد. سپس مارژین چمفر به شولدر ˚9...
background: although studies have shown that porcelain veneers are very effi cient for treating discolored teeth, they did not address in particular the minimum thickness of a multilayer ips e.max press (ivoclarvivadent, schaan, liechtenstein) restoration required to mask discolored tooth. the aim of this study was to determine the minimum thickness of a multilayer porcelain restoration require...
Purpose: The purpose of this in vitro study was to evaluate the effect simulated gastric acidity on surface roughness different types dental ceramics. Methods: Fifty specimens were divided according type material into five groups (n=10), as follows: Partially stabilized zirconia (PSZ) (Prettaue),Fully (FSZ) (Prettaue Anterior), lithium disilicate ceramics (IPS. Emax), Zirconia-containing silica...
سابقه و هدف: میزانmarginal gap در رستوریشن های تمام سرامیک در موفقیت این روکش ها اهمیت تعیین کننده ای دارد. با توجه به این که طرح تراش مارجین می تواند بر تطابق لبه ای تاثیرگذار باشد، هدف از این تحقیق مقایسه دو نوع طرح تراش shoulder وclassic chamfer بر تطابق لبه ای رستوریشن های تمام سرامیک ips e.max press در شرایط in vitro بود. مواد و روشها: این تحقیق به روش تجربی یک سوکور و به صورت in vitro انج...
مقایسه تطابق لبه ای سه سیستم ips empress2 ، ips e.max press و in ceram در رستوریشن های تمام سرامیکی دکتر عزت اله جلالیان1- دکتر مونا صادق2 - دکتر الهام حدادیان پور3 1- دانشیار گروه آموزشی پروتزهای ثابت دندانی دانشکده دندانپزشکی دانشگاه آزاد اسلامی 2- دستیار تخصصی گروه آموزشی اندودنتیکس دانشکده دندانپزشکی دانشگاه علوم پزشکی تهران 3- دندانپزشک چکیده زمینه و هدف : تطابق لبه ای در ر...