نتایج جستجو برای: in ceram alumina
تعداد نتایج: 16981531 فیلتر نتایج به سال:
This study investigated the influence of ceramic compositions on Knoop Hardness Number (KHN) immediately and 24 h after polymerization and the effect of activation modes on the KHN of a resin cement. Ten Panavia F 2.0 resin cement discs were activated either directly using curing light, or chemically without light, or through 1.2-thick ceramic discs. The following ceramics were evaluated: Ducer...
UNLABELLED Advances in all-ceramic systems have established predictable means of providing metal-free aesthetic and biocompatible materials. These materials must have sufficient strength to be a practical treatment alternative for the fabrication of crowns and fixed partial dentures. OBJECTIVES The aim of this study was to compare the biaxial flexural strength of three core ceramic materials....
OBJECTIVES The aim of this study was to evaluate the effect of mechanical cycling on the biaxial flexural strength of two densely sintered ceramic materials. METHODS Disc shaped zirconia (In-Ceram Zirconia) and high alumina (Procera AllCeram) ceramic specimens (diameter: 15 mm and thickness: 1.2 mm) were fabricated according to the manufacturers' instructions. The specimens from each ceramic ...
The aim of this study was to qualitatively demonstrate surface micro-morphological changes after the employment of different surface conditioning methods on high-alumina and glassy-matrix dental ceramics. Three disc-shaped high-alumina specimens (In-Ceram Alumina, INC) and 4 glassy-matrix ceramic specimens (Vitadur Alpha, V) (diameter: 5 mm and height: 5 mm) were manufactured. INC specimens wer...
The aims of this study were to evaluate the shear bond strength (SBS) of metal and ceramic brackets bonded to two different all-ceramic crowns, IPS Empress 2 and In-Ceram Alumina, to compare the SBS between hydrofluoric acid (HFA), phosphoric acid etched, and sandblasted, non-etched all-ceramic surfaces. Ninety-six all-ceramic crowns were fabricated resembling a maxillary left first premolar. T...
Aim: The aim of this study was to evaluate the micro shear bond strength of different ceramic systems IPS Empress 2, Cergogold, In-Ceram Alumina and Cercon and a dual luting agent. Methods: Twelve specimens of each ceramic were fabricated and divided according different surface treatments: Group 1: No additional treatment was applied to the ceramic surface; Group 2: Ceramics were etched with 9....
The aim of the present study was to evaluate the effect of thermocycling on the bond strength between the surface of the glass-infiltrated alumina ceramic In-Ceram (VITA) and the Panavia F resin cement (Kuraray CO.). Four 5x6x6mm In-Ceram blocks were obtained. One of the 6x6mm faces of each block was conditioned with Cojet - System (tribochemical silica coating, ESPE-3M) and then luted under a ...
UNLABELLED The development of all-ceramic systems following metalceramics restorations allowed simulation of natural dentition due to favorable esthetics and resistance. In-Ceram is an alternative when esthetics is primordial as well as resistance required in rehabilitation. However, an ideal smile is associated to not only shape, color, texture and translucency but also harmony with gingival t...
This study was conducted to enhance the tensile bond strengths of resin cements to zirconia ceramics. Fifty-six zirconia ceramic specimens (Cercon Base) and twenty-eight silica-based ceramic specimens (GN-1, GN-1 Ceramic Block) were air-abraded using alumina. Thereafter, the zirconia ceramic specimens were divided into two subgroups of 28 each according to the surface pretreatment; no pretreatm...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید