An AlZn4SiPb/steel clad composite was prepared via roll bonding at room temperature. The influence of solution and aging treatment on the structure performance investigated. results show that Al/steel composites exhibited satisfactory interfacial adhesion. Pb aged Al matrix spheroidized uniformly dispersed. uneven transition area with a thickness 30–150 nm observed for sample. Some rod-shaped n...
In this paper, an analytical model based on Modified Slab Method is presented for rolling of clad sheet or double-layers in which the two layers are bounded prior to rolling. This model considers the general case of asymmetrical rolling due to unequal 
surface speed, different contact friction, roll diameters, flow stress, and thickness ratios of the two layers. Using this model, rolling par...
In this paper, an analytical model based on Modified Slab Method is presented for rolling of clad sheet or double-layers in which the two layers are bounded prior to rolling. This model considers the general case of asymmetrical rolling due to unequal surface speed, different contact friction, roll diameters, flow stress, and thickness ratios of the two layers. Using this model, rolling param...
The nature and distribution of residual stresses are invariably critical for fatigue life with dissimilar material joints often inducing high tensile residual stresses. A fatigue-resistant concept of weld cladding process pipelines, producing compressive residual stresses, is under investigation to examine how these stresses may be influenced. Simplified weld cladding simulations have successfu...
Friction stir processing (FSP) was used as a cladding method for the fabrication of a AA2024 clad layer on a AA1050 sheet. Crossover multi pass FSP with 50% overlap was considered as the cladding method. Effects of the number of FSP passes and post heat treatment on the microstructure and properties of clad layers were evaluated. Microstructural evolutions during the FSP and heat treatment were...
The slurry erosion behaviour of laser clad Fe–Cr–B–Si alloy coatings was investigated at impact angles from 30u to 90u with an increment of 15u, and compared with the slurry erosion behaviour of two laser clad carbide coatings and a non-coated substrate made of AISI 4140 steel. The Fe–Cr–B–Si alloy coatings had slurry erosion resistance. Their overall slurry erosion resistance at impact angles ...
Two sodium-bonded, single phase (Uo.8PUo_2)C fueled. Type 316 stainless steel clad fuel elements were irradiated in EBR-II at heating rates of ~30 kW/ft to burnups of 3.7 and 5.0 at ." . No clad failures occurred as a result of the irradiation. Total fission gas release from the fuel was low. Thermal stresses in the fuel resulted in fuel splitting upon initial startup and general fuel fragmenta...