the effect of 6-month water storage on microleakage of two-component self-etch adhesive systems dr. mohammadibasir m .,1 dr. seyed tabaii e .2 1 assistant professor, department of operative dentistry , school of dentistry, shahed university. tehran , iran. 2 dentist. (received 5 dec, 2010 accepted 14 april, 2011) abstract background and aim : simplification of the self-etch...
Synthesis of boron-carbon-nitrogen (BCN) nanocarbon with a controllable bond structure for enhanced oxygen reduction reaction (ORR) activity and durability was performed using a new method of discharge in organic solution mixtures named the 'Solution Plasma Process'. Using selected precursors a new strategy for the simultaneous synthesis of nanocarbon co-doped with heteroatoms was found. The sy...
Background and Aim: Sodium hypochlorite can remove the organic phase of the demineralized dentin and it produces direct resin bonding with hydroxyapatite crystals. Therefore, the hydrolytic degradation of collagen fibrils which might affect the bonding durability is removed. The aim of this study was to evaluate the effect of collagen fibrils removal by 10% NaOCl on dentin shear bond strength o...
The aim of this study was to evaluate the effect of chlorhexidine (CHX) application on immediate and two-month bond strength of a filled adhesive system. Methods: Forty eight non-carious human third molars without enamel of occlusal surface were randomly divided into two main groups according to CHX application: control and CHX. Each main group was further subdivided into 2 subgroups depending ...
This study evaluated the influence of water storage conditions and the effect of metal priming agents on bond strength and durability of four luting agents joined to gold alloy. Disk specimens were cast from a gold alloy (Degudent U), and the surfaces were ground flat with abrasive paper. Three surface conditions employed were: unprimed, primed with Alloy Primer, and primed with Metaltite. Thre...
The lap shear strength of chromic acid anodized, primed, Ti-6Al-4V alloy bonded with a high performance FM-5 polyimide adhesive has been investigated as a function of thermal treatment for selected times at various temperatures in air. The research findings indicate that the lap shear strength decreases with the increase in duration of the thermal treatment at constant temperature and with the ...
The purpose of the present study is evaluation of bonding durability of tri-n-butylborane (TBB) initiated resin without 4-methacryloyloxyethyl trimellitate anhydride (4-META) joined to human enamel. Ground human enamel was bonded with TBB resin under six surface conditions: 1) as ground, 2) primed with Teeth Primer, 3) sodium sulfite solution, 4) 4-META solution, 5) acetone-water, and 6) phosph...
4-META/MMA-TBB resin has shown good biocompatibility and remarkable adhesion to dentin. It seems to be suitable for use in periodontal tissues for retrograde root sealing and treatment of vertically fractured roots. For an adhesive resin to be useful clinically, it must bond not only to the dentin but also to the cementum. The purpose of this study was to evaluate the long-term adhesion durabil...