2008

As shown in the preceding chapter, simple binary eutectic Ni-Hf and Ni-Zr braze alloys can be used to successfully join In738 Ni-base superalloy. The joint gap must, however, be narrow (less than 0.15 mm in width) to allow capillary action to draw the filler metal into the joint. Such narrow joint gaps are usually only found in the manufacturing industry. In the repair industry, especially in I...

2010
Bassam A. Abu-Nabah Waled T. Hassan Daniel Ryan Mark P. Blodgett Peter B. Nagy

Recent research results indicate that eddy current conductivity measurements can be exploited for nondestructive evaluation of subsurface residual stresses in surfacetreated nickel-base superalloy components. According to this approach, first the depth-dependent electric conductivity profile is calculated from the measured frequency-dependent apparent eddy current conductivity spectrum. Then, t...