To weaken the harm of Al–Si coating and increase strength welded joints, variable thicknesses Ni foil (Ni, an austenitic formation element) were added to lap laser welding Al–Si-coated 22MnB5 hot stamping steel/galvanized steel joints. The joints’ weld appearance, microstructure, mechanical properties explored. altered from X shape a Y with increased thickness foil. During welding, was melted d...