In this study, WC–20 wt.% equiatomic (Fe,Co) powder mixture was milled in a planetary ball mill. The effects of different milling time (15 min, 5h, 10h, and 25 h) and sintering temperatures on the microstructure and mechanical properties of this equi-Fe substituted cermet were investigated. The structural evolution and the crystallite size changes of the powders during milling were monitored by...
The aim of the present work is to study the effects of the nanostructured WC-20 wt. % (Fe,Co) with different ratios of iron to cobalt on the microstructure and hardness of sintered samples. Furthermore, a sample with a cobalt binder under the same condition was produced for the comparison purposes. The nanocomposite development, after different milling times, has been monitored by means of X-ra...
Silicon-doped (Si-doped) diamond films were deposited on a Co-cemented tungsten carbide (WC-Co) substrate using the hot filament chemical vapor deposition (HFCVD) method with a mixture of acetone, tetraethoxysilane (TEOS), and hydrogen as the recant source. The as-deposited doped diamond films were characterized with field emission scanning electron microscopy (FE-SEM), Raman spectrum, and X-ra...
Diamond coating of tungsten carbide-cobalt (WC-Co) cemented carbide tools using chemical vapour deposition (CVD) requires removal the cobalt (Co) binder phase from WC-Co surface in order to improve adhesion. Laser ablation is shown be a promising technique for selective Co, which based on difference melting and boiling temperatures between different phases. However, laser with conventional nano...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید