eaf plants normally consume coal and coke as reactants, alloying elements, or fuel. the price of these materials varies from € 0.20-0.35/kg. this is while nearly 10 million pieces of tires are annually discarded in iran. the present study shows that scrap tires can be used as a substitute for coal and coke in eaf plants. thirteen grades of steel including low, medium, and high carbon steels as ...
This study assessed whether there are differences in marginal fit between laser-fusion and conventional techniques to produce fixed dental prostheses (FDPs). A master steel die with 2 abutments was produced to receive a posterior 4-unit FDPs and single copings. These experimental models were divided into three groups (n = 20/group) manufactured: group 1, Ni-Cr alloy, with a lost-wax casting tec...
The aim of this research was to evaluate the effect of individual metallic elements within experimental Au-Pt-based metal-ceramic alloys on in vitro biocompatibility. A binary Au-10 at.% Pt alloy (AP10) was designed as a parent alloy. Six ternary AP10-X (X = In/Fe/Sn/Zn) alloys and four quaternary (AP10-In2)-Y (Y = Fe/Sn/Zn) with different compositions were cast into square plates with size 10X...
Structural, gaseous phase hydrogen storage, and electrochemical properties of a series of the Ti50Zr1Ni44X5 (X = Ni, Cr, Mn, Fe, Co, or Cu) metal hydride alloys were studied. X-ray diffraction (XRD) and scanning electron microscopy (SEM) revealed the multi-phase nature of all alloys, which were composed of a stoichiometric TiNi matrix, a hyperstoichiometric TiNi minor phase, and a Ti2Ni seconda...
Nickel-chromium (Ni-Cr) alloys used in fixed prosthodontics have been associated with type IV Ni-induced hypersensitivity. We hypothesised that the full-thickness human-derived oral mucosa model employed for biocompatibility testing of base-metal dental alloys would provide insights into the mechanisms of Ni-induced toxicity. Primary oral keratinocytes and gingival fibroblasts were seeded onto ...
The partial Wills-Harrison effective pair potentials in liquid equiatomic Co-Ni alloy are considered. It is shown that the account of the non-diagonal d-d couplings between electrons leads to similar changes in characteristics of the pair-potential first minimum as for Fe-Co and Fe-Ni equiatomic alloys.
Softcomag 49AA alloy consisting of 49 wt per cent Fe, 49 wt. per cent Co and 2 wt per cent V is a soft magnetic alloy with a combination of very high saturation magnetisation and high magnetostriction and used for several aeronautical applications such as generators (stators and rotors), fixed iron moving armature units etc. Though this alloy is brittle in nature, it can be formed into hot roll...
OBJECTIVE The shear bond strengths of two hard chairside reline resin materials and an auto-polymerizing denture base resin material to cast Ti and a Co-Cr alloy treated using four conditioning methods were investigated. MATERIAL AND METHODS Disk specimens (diameter 10 mm and thickness 2.5 mm) were cast from pure Ti and Co-Cr alloy. The specimens were wet-ground to a final surface finish of 6...
The goal of this study was to optimize the activation behaviour of hydrogen storage alloy TiFe. We found that the addition of a small amount of Zr in TiFe alloy greatly reduces the hydrogenation activation time. Two different procedural synthesis methods were applied: co-melt, where the TiFe was melted and afterward re-melted with the addition of Zr, and single-melt, where Ti, Fe and Zr were me...
Objectives Zirconia restorations have been suggested as a more durable and more appealing alternative to metal restorations. However, their mechanical properties may be negatively affected by fatigue due to superficial stresses or low temperature degradation. This study aimed to assess the fatigue fracture strength of three-unit implant-supported full contour zirconia and pre-sintered cobalt-ch...