MCM-41 was used as a support and, by using atomic layer deposition (ALD) in the liquid phase, a catalyst was prepared by consecutively loading titanium oxide and vanadium oxide to the support. This research analyzes the effect of the loading amount of vanadium oxide on the acidic characteristics and catalytic performance in the dehydration of butanol. The physical and chemical characteristics o...
Mesoporous silica materials (MSMs) of the MCM-41 type were rapidly synthesized by microwave heating using silica fume as silica source and evaluated as adsorbents for the removal of Cu2+, Pb2+, and Cd2+ from aqueous solutions. The effects of microwave heating times on the pore structure of the resulting MSMs were investigated as well as the effects of different acids which were employed to adju...
The interaction of water vapour with Al-MCM-41, prepared by direct synthesis at ambient temperature and pressure, using tetraethoxysilane, aluminium sulfate, hexadecyltrimethylammonium bromide and ammonia, and its effect on the pore structure were studied in order to investigate the stability towards prolonged exposure to water vapour and the influence of the aluminium content. With this purpos...
Pd nanoparticles were successfully introduced into the channels of mesoporous silica MCM-41 with their dispersion well-tuned. We identified the dual role played by CTAB, which was critical for both the micelle template and Pd grafting, leading to the formation of a highly active Pd-MCM-41 nanocomposite for catalysing the Suzuki reaction.
Anionic platinum carbonyl cluster has been ion paired with cinchonidium groups that are chemically bound to the surface of MCM-41 and fumed silica. In the hydrogenation of methyl pyruvate or acetophenone the fumed silica-based catalyst gives zero enantioselectivity, but under optimum conditions enantiomeric excesses of > 90 and ∼ 40%, respectively, are obtained with the MCM-41-based catalyst.
Catalytic pyrolysis behavior of synthesized microporous catalysts (conventional Zeolite Socony Mobil–5 (C-ZSM-5), highly uniform nanocrystalline ZSM-5 (HUN-ZSM-5) and β-zeolite), Mesoporous catalysts (highly hydrothermally stable Al-MCM-41 with accessible void defects (Al-MCM-41(hhs)), Kanemite-derived folded silica (KFS-16B) and well-ordered Al-SBA-15 (Al-SBA-15(wo)) were studied with waste po...
Several samples of mesoporous silica were prepared via sol-gel chemistry in the presence of CTAB as template with variation of stirring intensity and aging time, ratios of CTAB/SiO2 and NH4OH/H2O in synthesis mixture. Effects of aging temperature, hydrothermal treatment and ter-Butanol addition to the synthesis mixture on the textural properties of obtained samples were also studied. Results of...
Ti-MCM-41 was synthesized at pH 3, 7 and 11. The titanium content was determined by AAS and found to be 4%, 3.2% and 4.5%, respectively. In order to increase the titanium content in Ti-MCM-41, Ti(IV) ions were grafted onto TiMCM-41 using TiCl4 in toluene and Ti(OBu)4 in ethanol. The incorporation of Ti was determined to be 28% and 30%, respectively. The oxidation of olefins such as cyclopentene...