A resorcinol resin/water dispersion and a rubber latex are added to 1% 2,2,6,6,-tetramethylpyperidine-1-oxyl (TEMPO)-oxidized cellulose nanofibers (TEMPO-CNFs) dispersed in water, followed by oven drying at 40 °C for 20 h prepare dried TEMPO-CNF/resorcinol resin/latex (DTRL) mixture with weight ratio of 1/0.5/3. DTRL is then nitrile-butadiene (NBR) or carboxy group-containing NBR (X-NBR) sheet,...