This research developed new nanostructured Al–Fe3O4 composites via accumulative roll bonding (ARB). X-ray diffraction (XRD) analysis and field emission scanning electron microscopy were conducted to examine microstructural characteristics and particle distribution in the nanocomposites. Hardness and tensile strength tests were employed to examine their mechanical propertie...
PBXN-111 is a common plastic bonded explosive has been widely used in warhead section of several navy weapons. This charge is based on HTPB resin and prepared with cast-cure method. Isodecyl pelargonate (IDP) as plasticizer is used in PBXN-111 formulation. Considering limitations to prepare IDP, in this research the effect of replacement of dioctyl adipate (DOA) and dioctyl sebacate (DOS) inste...
In this research, the effect of bonding temperature on the microstructure and mechanical properties of Inconel 939 super alloy by transient liquid phase bonding method. For this purpose, the middle layer of MBF20 with a thickness of 50 microns and three temperatures of 1060 °C, 1120 °C, 1180 °C and a time of 45 minutes have been used. In order to evaluate the microstructure, a scanning electron...
Polyvinyl ester green composites were synthesized with walnut shell powder (WSP) by in-situ polymerization technique. The green composites have been evaluated for mechanical properties such as tensile strength, tensile modulus and hardness. Sliding wear loss, specific wear rate and coefficient of friction were investigated by using computerized pin-on–disc machine at normal applied loads of 20,...
Present study focuses on the micro-structural and mechanical behavior effect of friction time for similar (AISI 316-AISI 316 and AISI 304-AISI 304) and dissimilar (AISI 304-AISI 316) joint during continuous drive friction welding. The welding carried out with different friction time: 6.5, 8.5 and 10 s while kept all other conditions constant. The effect of that time on the strength, structural ...
In this study, an industrial polycrystalline SiC tile was successfully sintered by pressureless sintering at 2150°C for 1 hour. The physical and mechanical properties of silicon carbide including density, hardness, bending strength, and fracture toughness were evaluated. The results indicated that the mentioned properties were 3.08 g.cm-3, 2503 HV0, 249.3 MPa, and 1.23 MPam0.5</...
In this research, the effect of bonding temperature on the microstructure and mechanical properties of Inconel 939 super alloy by transient liquid phase bonding method. For this purpose, the middle layer of MBF20 with a thickness of 50 microns and three temperatures of 1060 °C, 1120 °C, 1180 °C and a time of 45 minutes have been used. In order to evaluate the microstructure, a scanning electron...
Solid-state direct diffusion bonding of commercially pure Titanium (Cp-Ti) and precipitation hardening stainless steel (PHSS) has been carried out in the temperature range of 800°C to 1000°C with an interval of 50°C for 3.6 ks under 3.5 Mpa uniaxial load in (4 to 6)×10 Pa vacuum. The effects of temperatures have been investigated with reference to bond strength. The examination revealed that th...
Porous NiTi alloys were prepared by microwave sintering using ammonium hydrogen carbonate (NH4HCO3) as the space holder agent to adjust the porosity in the range of 22-62%. The effects of porosities on the microstructure, hardness, compressive strength, bending strength, elastic modulus, phase transformation temperature and superelasticity of the porous NiTi alloys were investigated. The result...