Due to the unique hydrothermal environments, frost heave failure of concrete lining water conveyance canals in cold regions is still frequent. The deformation after heaving and stress distribution calculated by mechanical model can be reference for design. However, previous research mainly focused on cross-section while having little attention longitudinal nonuniform damage. In this study, a bo...