نتایج جستجو برای: bonding strength

تعداد نتایج: 245343  

Ali Heidari, Ali Nozari, Azade Rafiee,

Introdouction: Esthetic demands of patients have led to the introduction of tooth-colored restorations wherecomposite resins are bonded to the enamel using acid etch techniques. Total etch adhesion systems are still considered as the gold standard among bonding systems. However, clinicians have a tendency to use adhesive systems with simpler application procedures. The aim of the present stu...

Farideh Darabi, Hanieh Dadashi, Reza Tayefeh Davalloo, Seyedeh Maryam Tavangar, Yasaman Sadeghi, Zahra Atrkar Roushan,

Introduction: To evaluate and compare shear bond strength of self-cure and  light-cure composites using a universal bonding system. Materials and Methods: Superficial coronal dentin of 62 intact extracted  premolars was exposed and bonding agent (All-Bond Universal) was applied over the  dentin surface according to the manufacturer instruction (self-etch mode). Then  samples were distribut...

Journal: :Bulletin of the Japan Institute of Metals 1986

Journal: :Quintessence international 2009
Bilge Tarçin Mahir Günday Hesna S Oveçoğlu Cafer Türkmen M Lütfi Oveçoğlu Mustafa Oksüz Mustafa Ay

OBJECTIVE To evaluate tensile bond strengths of 2 dentin bonding agents containing solvents on Nd:YAG and Er,Cr:YSGG laser-etched dentin surface. METHOD AND MATERIALS Occlusal enamel of 146 molars was removed, and exposed surfaces were ground with a diamond bur to produce bur-cut dentin surfaces. Of those teeth, 120 were assigned to 3 groups of 40 samples in which dentin was conditioned with ...

2017
Mizuho KUSUNOKI Kazuo ITOH Yoiehi TAKAHASHI Mizuho Kusunoki

To evaluate the effect of a dentin adhesive on sclerotie dentin, contraetion gap width and shear bond strength were measured, Dent{n cavity wall was pretreated with an experimental dentin bonding system w{th and without a dentin primer, or with a commercial dentin bonding system. In the experimental dentin bonding groups, contraction gap width of sclerotic dentin was signifieantly smaller than ...

2015
Ho-Jin Moon

Regardless of bleaching regimes, the bond strength of composite resin or resin cement is reduced when bonding procedure is performed immediately after whitening. It is believed that the polymerization via free-radical mechanism is impeded by nascent oxygen remnant and peroxide in the bleached dental hard tissue. Because sodium hydroxide is used as a buffering agent to control the decreased pH, ...

2004
K. N. Chen C. S. Tan A. Fan R. Reif

The morphology and bond strength of copper-bonded wafer pairs prepared under different bonding/annealing temperatures and durations are presented. The interfacial morphology was examined by transmission electron microscopy (TEM) while the bond strength was examined from a diesaw test. Physical mechanisms explaining the different roles of post-bonding anneals at temperatures above and below 300°...

Ali Davoodi, Mohammad Javad Kharrazifard, Sima Shahabi, Stefano Benedicenti, Zahra Amiri,

Background and Aim: Bonding of zirconia to resin cement is challenging, and the zirconia surface requires surface treatment to yield an acceptable bond strength. This study aimed to evaluate the effect of different surface treatments on the bond strength of zirconia to a resin cement. Materials and Methods: In this in-vitro experimental study, 60 zirconia discs measuring 12 mm in diameter an...

Journal: :Dental materials journal 2006
Alp Erdin Koyuturk Abdulkadir Sengun Fusun Ozer Yagmur Sener Alparslan Gokalp

The purpose of this study was to evaluate the bonding ability of five current self-etching adhesives to caries-affected dentin on the gingival wall. Seventy extracted human molars with approximal dentin caries were employed in this study. In order to obtain caries-affected dentin on the gingival wall, grinding was performed under running water. Following which, specimens mounted in acrylic bloc...

Mirsalehi, S. E. , Shamsipoor, A. , Tazikeh, H. ,

In this research, the effect of bonding temperature on the microstructure and mechanical properties of Inconel 939 super alloy by transient liquid phase bonding method. For this purpose, the middle layer of MBF20 with a thickness of 50 microns and three temperatures of 1060 °C, 1120 °C, 1180 °C and a time of 45 minutes have been used. In order to evaluate the microstructure, a scanning electron...

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید