Sintered bodies of Zr2WP2O12 (ZWP) and ZrV0.6P1.4O7 (ZVP) were fabricated, and their linear thermal expansion coefficients (TEC) were found to be -2.92 × 10-6 and 3.27 × 10-6 °C-1, respectively, in the range 25-500 °C. In an attempt to fabricate composites with a zero-thermal-expansion property, sintered ZWP/ZVP composites with ZVP/ZWP volume ratios of 0.5/0.5, 0.53/0.47, 0.55/0.45, and 0.6/0.4...