2008
D. W. Kim R. S. Qin H. K. D. H. Bhadeshia

Many aspects of the crystallographic texture which develops when austenite transforms into martensite or bainite are well established because the process by which the parent lattice is transformed into that of the product is mathematically defined. This is not the case when the ferrite forms by a reconstructive mechanism. The allotriomorphic ferrite nucleates heterogeneously at austenite grain ...

2004
M. Peet S. S. Babu M. K. Miller H. K. D. H. Bhadeshia

A bainitic microstructure with fine ferrite plates (20 to 40 nm) in a matrix of high-carbon retained austenite, obtained by isothermal transformation at 200°C, was characterized with an energy-compensated optical position-sensitive three-dimensional atom probe. The average carbon concentration in the austenite was found to be 8.0±1.6 at.% and in the bainitic ferrite 1.1±0.7 at.%. The latter con...

Journal: :Acta Metallurgica Sinica (english Letters) 2021

By tailoring the reverse austenite transformation behavior of 9Cr oxide dispersion strengthened (ODS) ferritic/martensitic steels, residual ferrite in ODS steels can be controlled. The is closely related to initial microstructure conditions prior transformation. For spark plasma sintered both amount and size decrease with increasing heating rate. Nevertheless, high rate will increase annealed s...

2016
S. GANGADHARAN

Brazing of an austenitic-martensitic stainless steel (AMSS) with pure silver was carried out at 1053 K, 1073 K, and 1093 K (780 C, 800 C, and 820 C) with Ag-27Cu-5Sn (wt pct) as brazing filler material (BFM). Wettability of the liquid BFM over base AMSS surface was found to be poor. Application of nickel coating to the steel was observed to enhance the wettability and to enable the formation of...

2005
B. K. Tay Z. W. Zhao C. Q. Sun

Two sets of aluminium oxide thin films were deposited using off-plane filtered cathodic vacuum arc (FCVA) at the working pressure of 6 10 4 Torr under various substrate biases ( 60 to 140 V) and substrate temperatures (120–600 8C), respectively. Optical and mechanical properties, such as refractive index, residual stress, hardness and Young’s modulus, of the films were investigated. It has been...

2014
Pravin M. Kulkarni

Hybrid Layered Manufacturing (HLM) combines the benefits of both subtractive and Additive Manufacturing (AM). In this paper authors did characterization of AM components by using Kernel Average Misorientation (KAM), Electron Backscatter Diffraction (EBSD) and hardness tester. The main focus is on matrix integrity during Gas Metal Arc Welding (GMAW) deposition and surface quality during machinin...

2008
E. Jimenez-Melero N. H. van Dijk L. Zhao J. Sietsma S. E. Offerman J. P. Wright S. van der Zwaag

We have performed in situ synchrotron X-ray diffraction experiments to assess the influence of aluminium and phosphorus on the austenite stability in low-alloyed transformation-induced plasticity steels during the high-temperature bainitic holding and the subsequent martensitic transformation during cooling to temperatures between room temperature and 100 K. Although the addition of aluminium i...

2007
S. S. Babu E. D. Specht S. A. David E. Karapetrova P. Zschack M. Peet H. K. D. H. Bhadeshia

In-situ time-resolved X-ray diffraction technique with synchrotron radiation was used to track austenite decomposition in steels. Measurements from a Fe-C-Si-Mn steel indicate two lattice parameters in the austenite, possibly due to the development of carbon-rich and carbon-poor austenite prior to transformation. The lattice parameter became uniform with the progress of transformation and the f...

2001
A. L. McKELVEY

This article presents a study of fatigue-crack propagation behavior in Nitinol, a 50Ni-50Ti (at. pct) superelastic/shape-memory alloy, with particular emphasis on the effect of the stress-induced martensitic transformation on crack-growth resistance. Specifically, fatigue-crack growth was characterized in stable austenite (at 120 8C), superelastic austenite (at 37 8C), and martensite (at 265 8C...