The effects of stress and plastic strain distributions on the hydrogen embrittlement fracture U-bent martensitic steel sheet specimen were investigated. testing was performed. Fracture morphology mainly consisting intergranular found inside charged specimen, which indicated that crack initiation took place in interior, shear lips near both surfaces sheet. synchrotron X-ray diffraction measureme...