نتایج جستجو برای: nickel zinc ferrite

تعداد نتایج: 111244  

2016
Shiwei Zhou Yonggang Wei Bo Li Hua Wang Baozhong Ma Chengyan Wang

Sodium chloride has been proved that it is an effective promoter for the reduction of high-magnesium, low-nickel oxide ore. The aim of current work is to clarify the promotion behavior of sodium chloride in the roasting reduction process. The influence of moisture on the reduction of ore in the presence of sodium chloride is studied to get clear comprehension of promotion process. In the presen...

The present study aims to identify the impact of polluted aquatic body i.e. River Hindon on two selected riparian flora i.e. Azadirachta indica and Acacia nilotica. During the course of study the average concentration of different metals in river water was found as Iron (Fe) 11.27ppm±3.50, Manganese (Mn) 4.00ppm±1.26, Cadmium (Cd) 0.08ppm±0.07, Nickel (Ni) 0.63ppm±0.17 and Zinc (Zn) 1.46ppm±0.3...

Journal: Pollution 2019

The present study aims to identify the impact of polluted aquatic body i.e. River Hindon on two selected riparian flora i.e. Azadirachta indica and Acacia nilotica. During the course of study the average concentration of different metals in river water was found as Iron (Fe) 11.27ppm±3.50, Manganese (Mn) 4.00ppm±1.26, Cadmium (Cd) 0.08ppm±0.07, Nickel (Ni) 0.63ppm±0.17 and Zinc (Zn) 1.46ppm±0.3...

Journal: :iranian journal of chemistry and chemical engineering (ijcce) 1995
mohammad hossein arbab zavar maryam kazemipour

lead, copper, cobalt, nickel, iron and zinc ions form monocitrate complexes (negative charge) in citrate solution which is absorbed on the citrate form of anion-exchange resins (citrate as counter ion) y exchange of citrate ion with citrate complexes. these are subsequently recovered from the resin by 0.5m ammonium citrate eluent at ph 2.0. under optimized conditions, quantitative recovery was ...

برقعی, مهدی, عموئی, عبدالایمان , فرجی, حسین, محسنی, مجید, گودرزی, جواد,

Background and purpose: Heavy metals such as chromium, nickel, and zinc are the most common contaminants found in the plating wastewater that cause environmental pollution due to non-biodegradability. This study investigated the removal of chromium, nickel, zinc and turbidity from wastewater of plating and galvanized industries by electrocoagulation technology. Material and methods: This study...

2017
J. Tasaki T. Izushi J. TASAKI

The influence of various cations ranging from alkali metals to transition metals according to the periodic table were discussed. The ferrites used were Ni ferrite, Mg ferrite and Zn ferrite having different cation distributions in the spinel lattice. Cations having appropriate ionic radii and valencies are soluble in ferrite. Several additives formed other phase in addition to the spinel phase....

2008
Carlos Bárcena Amandeep K. Sra Girija S. Chaubey Chalermchai Khemtong J. Ping Liu Jinming Gao

Magnetic resonance imaging (MRI) is a powerful clinical imaging technique for the non-invasive diagnosis and posttherapy assessment of a variety of diseases. MRI contrast can be enhanced by the use of positive or negative contrast agents resulting in brighter (T1-weighted) or darker (T2-weighted) images, respectively. Superparamagnetic iron oxide (SPIO) nanoparticles are T2 contrast agents that...

2016
V. Brabers

Highly stoichiometric zinc ferrous ferrites Zn,F+,O, were prepared and characterized by magnetization, desacwmmodation, electrical conductivity, thermal expansion and magnetostriction measurements. The results of the magnetization measurements indicate that up till x = 0.5 the magnetic structure is collinear, which led to the highest saturation magnetizations ever found in spinel femtes. The th...

2008
E. M. K. Hillier M. J. Robinson

Slow strain rate tests were performed on quenched and tempered AISI 4340 steel to measure the extent of hydrogen embrittlement caused by electroplating with zinc-cobalt alloys. The effects of bath composition and pH were studied and compared with results for electrodeposited cadmium and zinc-10%nickel. It was found that Zinc-1%cobalt alloy coatings caused serious hydrogen embrittlement (EI 0.63...

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید