Journal: :Dental materials journal 2005
Tetsuya Suzuki Hidekazu Takahashi Mansuang Arksornnukit Nobusuke Oda Shigezo Hirano

The purpose of this study was to evaluate the shear bonding strength and leakage of heat-polymerized denture base resin to titanium-aluminum-niobium (Ti-6Al-7Nb) and cobalt-chromium (Co-Cr) castings using four adhesive systems; three adhesive primers (Metal Primer II, Metal Link, MR. Bond) and one heat-polymerized adhesive resin containing 4-META (Metadent). The resin tab was heat-polymerized d...

Journal: :Dental materials journal 2007
Takashi Tsuruoka Yasuhiro Namura Noriyoshi Shimizu

We produced experimentally a new bonding material that consisted of a mixture of a base resin (4-META/MMA-TBB resin adhesive) and thermoexpandable microcapsules for safe, easy debonding. Microcapsules in the base resin would start expansion at 80 degrees C, leading to a remarkable decrease in bond strength. Stainless steel brackets were bonded to bovine permanent mandibular incisors using bondi...

2004
C T Pan

In this study, a new technique of selective microcap bonding for packaging 3-D MEMS (Micro Electro Mechanical Systems) devices is presented. Microcap bonding on a selected area of the host wafer was successfully demonstrated through flip chip and wafer level alignment. A passivation treatment was developed to separate the microcap from the carrier wafer. A thick metal nickel (Ni) microcap was f...

2017
Hailiang Yu Cheng Lu Kiet Tieu H. L. Yu C. Lu A. K. Tieu C. Kong

In this paper, an extended accumulative roll bonding (ARB) technique, called the 'Four-Layer Accumulative Roll Bonding (FL-ARB)' technique, is presented for the first time. This technique has been employed to produce ultrafine-grained commercial pure aluminum sheets with success. After three FL-ARB passes, the grain size of pure aluminum was seen to reduce to 380 nm. The bonding strength of the...

Journal: :Journal of the Surface Finishing Society of Japan 1989

Journal: :Science and technology of advanced materials 2012
Takahito Inoue Tetsushi Taguchi Shinji Imade Nobuyuki Kumahashi Yuji Uchio

We have investigated the effectiveness and safety of a newly developed biological adhesive for repair of meniscal tear. The adhesive was composed of disuccinimidyl tartrate (DST) as a crosslinker and human serum albumin (HSA) as a hardener. To determine adequate concentration, bonding strength was measured using a tensiometer 5 min after applying the adhesive on the avascular zone tear of porci...

2013
Fulya Ozdemir Umut Cakan Nese Gonul Derya Germec Cakan

OBJECTIVE Bonding forces of brackets to enamel surfaces may be affected by the procedures used for bleaching and enamel etching. The aim of this study was to investigate the bonding strength of orthodontic brackets to laser-etched surfaces of bleached teeth. METHODS In a nonbleached control group, acid etching (group A) or Er:YAG laser application (group B) was performed prior to bracket bond...

Journal: :IEICE Transactions 2016
Eiji Higurashi Michitaka Yamamoto Takeshi Sato Tadatomo Suga Renshi Sawada

Low-temperature bonding methods of optoelectronic chips, such as laser diodes (LD) and photodiode (PD) chips, have been the focus of much interest to develop highly functional and compact optoelectronic devices, such as microsensors and communication modules. In this paper, room-temperature bonding of the optoelectronic chips with Au thin film to coined Au stud bumps with smooth surfaces (Ra: 1...

ژورنال: مجله دندانپزشکی 2017

Background and Aims: Poor adhesion between porcelain and some of the dental alloys is one of the most challenges to select the desirable alloy in dental restorations. Therefore, the aim of this study was to evaluate the bond strength of porcelain to some of the commercial alloys. This can help in selection of desirable alloy. Materials and Methods: The shear bond strength of porcelain to the t...