Pure serum amyloid P component (SAP) and native long chromatin, mixed together at wt/wt ratios between 1:1 and 1:2 in the presence of physiological concentrations of NaCl and calcium, both remained in solution, whereas each alone precipitates rapidly under these conditions. This solubilization accompanies the binding of SAP to chromatin and the displacement of H1-type histones, which are essent...
in the present study, ni-p-cnt composite coating was successfully fabricated via electroless plating. scanning electron microscopy (sem) was used to characterize the coatings. the effect of cnts concentration in the bath on its content in the composite coatings was studied. furthermore, the corrosion behaviour of the coatings with different contents of cnts was evaluated using tafel polarizatio...
A great challenge in wastewater bioremediation is the sustained activity of viable microorganisms, which can contribute to the breakdown of waste contaminants, especially in alkaline pH conditions. Identification of extremophiles with bioremediation capability can improve the efficiency of wastewater treatment. Here, we report the discovery of an electrochemically active alkaliphilic halotolera...
The effect of Al on the corrosion resistance behaviour of Pb-free Sn–1.0Ag–0.5Cu–xAl solder (x 1⁄4 0.2 wt%, 0.5 wt% and 1.0 wt%) in 5% NaCl solution was investigated by using potentiodynamic polarization and salt spray exposure. Passivation behaviour was evident in all the solder formulations containing Al, compared to the base SAC solder. FESEM and XRD results revealed that more dense passive ...
Lactobacillus curvatus LTH 1174, a strain originating in fermented sausage, produces the antilisterial bacteriocin curvacin A. Its biokinetics of cell growth and bacteriocin production as a function of various concentrations of salt (sodium chloride) were investigated in vitro during laboratory fermentations using modified MRS medium. A model was set up to describe the effects of different NaCl...
In this work, Slow Strain Rate Test (SSRT) testing, Light Optical Microscopy (LOM) and Scanning Electron Microscopy (SEM) were used to study the effect of microstructure, corrosive environments and cathodic polarisation on stress corrosion cracking (SCC) of two grades of high strength steels, Type A and Type B. Type A is manufactured by quench and tempered (Q&T) method. Type B, a normalize stee...
Abstract 30MnB5 boron alloyed steel surface is coated using different coating techniques, namely 60(Ni-15Cr-4.4Si-3.5Fe-3.2B 0.7C)-40(WC 12Co) metallic powder plasma spray, Fe-28Cr-5C-1Mn alloy wire arc WC-10Co-4Cr (thick) high velocity oxy-fuel (HVOF), and (fine) diamond jet HVOF. The microstructure of the crude sample consists ferrite pearlite matrices iron carbide structures. intermediate bi...
Water intakes in response to hypertonic, hypovolemic, and dehydrational stimuli were investigated in mice lacking angiotensin II as a result of deletion of the angiotensinogen gene (Agt-/- mice), and in C57BL6 wild-type (WT) mice. Baseline daily water intake in Agt-/- mice was approximately threefold that of WT mice because of a renal developmental disorder of the urinary concentrating mechanis...
In this study, vanadium conversion coating(VCC) was deposited on the surface of soft-cast steel (St-37). A thermoset coating was enforced on the VCC and blank substrates. The surface was characterized by field emission scanning electron microscope (FE-SEM), elemental mapping of energy dispersive X-ray (EDX) and atomic force microscopy (AFM). The adhesion strength...