The microstructure and mechanical properties of an MMC based on AA 7075 strengthened through silicon carbide (SiC) as well boron (B4C) elements were studied. (SiC + B4C) combination was used in various weight percentages 4, 8, 12, 16% to create the hybrid composites utilizing traditional stir casting procedure. XRD SEM measurements investigate dispersion reinforced particles. For example, micro...