نتایج جستجو برای: tungsten carbide

تعداد نتایج: 19500  

Journal: :Bulletin of Materials Science 1986

Journal: :Journal of computational chemistry 2010
Erjun Zhao Jinping Wang Zhijian Wu

The structural stability and phase transition of osmium and ruthenium carbides (OsC and RuC) were investigated by first principles. Nine structures were considered for each carbide. Zinc blende structure has the lowest energy among the considered structures at ambient conditions for both carbides. For OsC at elevated pressures, the most stable phase is zinc blende structure from 0 to 10 GPa, Fe...

2007
C. M. Fernandes

Composite powders of tungsten carbide with variable coating contents of Fe/Ni/Cr based alloys (1–15 wt.%) were prepared by sputtering. The coated powders have revealed a good performance to shape-forming and sintering. However, the presence of nanocrystalline coatings could enhance the formation of a brittle phase during sintering, named g-phase, (M,W)6C. To investigate this effect, the powders...

F. Ashrafizadeh F. Madadi M. Shamanian,

This paper deals with the investigation of the microstructure and hardness of steel samples cladded with satellite 6-WC composites by using gas tungsten arc welding (GTAW) process. For this purpose, steel samples were coated with unreinforced and reinforced stellite (by 20, 30 and 40 wt.% WC). The cladded samples were evaluated by metallographic studies, microhardness measurement and X-ray diff...

2007
H. Yu R. Ahmed H. de Villiers Lovelock

This paper aims to compare the tribo-mechanical properties and structure–property relationships of a wear resistant cobalt-based alloy produced via two different manufacturing routes, namely sand casting and powder consolidation by hot isostatic pressing (HIPing). The alloy had a nominal wt % composition of Co–33Cr–17.5W–2.5C, which is similar to the composition of commercially available Stelli...

Journal: : 2021

In this research work we have coated WC (tungsten carbide) tool inserts with diamond like carbon coatings. The deposition was done using the thermal Chemical Vapour Deposition (CVD) method. We used bagasse of sugarcane which is an agriculture waste as a precursor for developing Surface finish, cutting temperature and forces as-developed coatings on were examined analyzed in work. For confirming...

2014
Xiaoyong Ren Zhijian Peng Zhiqiang Fu Chengbiao Wang

Ultrafine tungsten carbide-nickel (WC-Ni) cemented carbides with varied fractions of silicon carbide (SiC) nanowhisker (0-3.75 wt.%) were fabricated by spark plasma sintering at 1350°C under a uniaxial pressure of 50 MPa with the assistance of vanadium carbide (VC) and tantalum carbide (TaC) as WC grain growth inhibitors. The effects of SiC nanowhisker on the microstructure and mechanical prope...

2011
Do-Heyoung Kim Young Jae Kim Yo Soon Song Byung-Teak Lee Jin Hyeok Kim Seigi Suh Roy Gordon

Tungsten carbide (WCx) thin films were prepared by plasma-assisted atomic layer deposition ALD using bis tertbutylimido bis dimethylamido tungsten at 250°C. The effects of plasma pulse time, radio frequency power, and the N2 /H2 ratio on the film properties, such as resistivity, surface roughness, step coverage, and stability in air, were examined. The film growth rate thickness/cycle was in th...

Journal: :Nanoscale 2015
Wenjing Fang Allen Hsu Yong Cheol Shin Albert Liao Shengxi Huang Yi Song Xi Ling Mildred S Dresselhaus Tomas Palacios Jing Kong

We have found that tungsten (W) foils can be used for controlling the carbon diffusion within copper (Cu) enclosures to synthesize large-domain bi-/multi-layer-free monolayer graphene via chemical vapor deposition. We have observed that bi-/multi-layer graphene that nucleate underneath the monolayer graphene can be selectively removed by a W foil placed inside of the Cu enclosure. Both X-ray ph...

The aim of this investigation is obtaining WC-Co composite powder from WO3 and Co3O4 by in-situ and carbothermic reduction method using activated carbon as a reducing agent. In this study, cobalt and tungsten oxide powders with 17% carbon (30% more than stoichiometric value) were mixed by ball-milling under atmosphere of argon for 20 hours. Differential Thermal Analysis (DTA) and Therm...