Although nanoscale twinning is an effective means to enhance yield strength and tensile ductility in metals, nanotwinned metals generally fail well below their theoretical strength limit due to heterogeneous dislocation nucleation from boundaries or surface imperfections. Here we show that Au nanowires containing angstrom-scaled twins (0.7 nm in thickness) exhibit tensile strengths up to 3.12 G...
Spontaneous bilateral mode II shear ruptures were nucleated on faults in photoelastic Homalite plates loaded in uniaxial compression. Rupture velocities were measured and the interaction between the rupture front and short fault branches was observed using high-speed digital photography. Fault branches were formed by machining slits of varying lengths that intersected the fault plane over a ran...
Magnesium alloys have recently attracted great interest due their lightweight and high specific strength. However, because of their hexagonal close-packed structure, they have few active slip systems, resulting in poor ductility and high mechanical anisotropy at room temperature. In the present work, we used a cross-shear deformation imposed by a differential speed rolling (DSR) technique to im...
The mechanical properties of dentin are changed after bleaching, although the effects of the bleaching conditions on the tensile strength of dentin have not been determined. In the current study, a tensile test of bovine dentin was conducted after bleaching and the effects of the bleaching conditions were investigated, including the number of bleaching times, the location where the bleaching ag...
During the brazing of aluminum-based heat exchangers, the flux dry-off temperature plays a crucial role to get sound joints with maximum strength. In the present study, the NOCOLOK® flux consists of two phases of K2AlF5.H2O and KAlF4 with a melting point around 580 °C was used for brazing AA3003 as base metal with a clad-coating of AA4343 as filler metal. The slurry was applied on the joints an...
During the brazing of aluminum-based heat exchangers, the flux dry-off temperature plays a crucial role to get sound joints with maximum strength. In the present study, the NOCOLOK® flux consists of two phases of K2AlF5.H2O and KAlF4 with a melting point around 580 °C was used for brazing AA3003 as base metal with a clad-coating of AA4343 as filler metal. The slurry was applied on the joints an...
Diametral compression tests were performed on pultruded composite rods comprised of unidirectional glass or carbon fibers in a common matrix. During compression tests, acoustic emission (AE) activity was recorded and images were acquired from the sample for analysis by digital image correlation (DIC). In both composite systems, localized tensile strain developed in the transverse plane under th...
failure in timber structures occurs mainly in crucial points such as joints areas. therefore, the idea of using composite sheets in timber joints has been intro-duced as a method in order to increase the strength and ductility behaviour of timber joints. this research aims to study the behaviour of bolted joints in poplar and pine woods, which are reinforced by two types of gfrp sheets. a singl...