INTRODUCTION New materials can increase the efficiency of pulp capping through the formation of a complete reparative dentin bridge with no toxic effects. The present study involved tomographic evaluations of reparative dentin bridge formation after direct pulp capping with calcium hydroxide, mineral trioxide aggregate (MTA), Biodentine (Septodont, Saint Maur des Fossés, France), and Single Bon...
This study verified the optical density of four composite resin luting agents - RelyX ARC (RY), Enforce (E), C&B Cement (CB) and Flow it (FI), at thicknesses of 2, 3, and 4 mm. The optical density of the luting agents was compared with that of enamel and dentin at the same thicknesses. Fifteen tooth crowns were embedded in PVC cylinders with self-cured acrylic resin. In addition, acrylic resin ...
statement of problem: adhesion to root canal dentin is one of the necessary characteristics of endodontic sealers. mta fillapex (angelus, londria, pr, brazil) is one of the recently introduced mta-based sealer. only a limited number of studies have evaluated the bonding of this sealer to the dentin, with conflicting results. objectives: the purpose of this study was to evaluate the bond strengt...
OBJECTIVES To evaluate the effect of Fe₂O₃on the optical properties of yttria-stabilised tetragonal zirconia (Y-TZP) dental ceramic when added, and to determine the correct content required to mimic the natural dentin. METHODS Disc-shaped Y-TZP specimens (0.50 ± 0.01 mm in thickness) containing various contents of Fe₂O₃were fabricated by cold isostatic pressing and pressureless sintering, and...
PURPOSE The purpose of this investigation was to study in-vitro the attachment behavior of human periodontal ligament (HPDL) fibroblasts to nondemineralized dentin surface using scanning electron microscope. STUDY DESIGN Thirty root slices of freshly extracted human teeth of 4 mm thickness as well as six 5x5 mm glass slides used as a control were used in this study. The dentin surface of the ...
Abstract BACKGROUND AND OBJECTIVES: The purpose of this study was to analyze the microstructural changes caused by Carisolv gel on sound, demineralized, and denatured dentin. METHOD: A total of 48 freshly extracted human premolars and molars were collected and divided into 3 main groups, Group I contained 12 teeth with fractured dentinal surface, which were further divided into two subgroups IA...
comparison of microleakage and thickness of resin cement in ceramic inlays with various temperatures
background and aims. microleakage is still one of the major problems of composite-based restorations. this study compared the microleakage and thickness of resin cement in ceramic inlays with various temperatures. materials and methods. class v cavities were prepared on the buccal and lingual aspects of thirty human molars with occlusal margins in enamel and gingival margins in dentin (3 mm wid...
OBJECTIVE In this investigation the thickness of enamel in the gingival, middle, and incisal thirds of the labial surface of the anterior teeth were measured regarding preparation of the teeth for porcelain laminate veneers. MATERIALS AND METHODS Part one, 20 extracted intact human maxillary central and lateral incisors ten of each were selected. The teeth were imbedded in autopolimerize acry...
Plasma and halogen lamp units were used to photo-cure a composite resin for porcelain bonding. Mean shear bond strengths to dentin after light curing through porcelain of 1 and 2 mm thickness ranged from 20 to 27 MPa before and after thermocycling, indicating no significant effects due to porcelain thickness, curing method, or thermocycling, except for plasma curing for 3 s through porcelain of...