Journal: :Dental materials : official publication of the Academy of Dental Materials 2008
Dolores R R Lazar Marco C Bottino Mutlu Ozcan Luiz Felipe Valandro Regina Amaral Valter Ussui Ana H A Bressiani

OBJECTIVES (1) To synthesize 3mol% yttria-stabilized zirconia (3Y-TZP) powders via coprecipitation route, (2) to obtain zirconia ceramic specimens, analyze surface characteristics, and mechanical properties, and (3) to compare the processed material with three reinforced dental ceramics. METHODS A coprecipitation route was used to synthesize a 3mol% yttria-stabilized zirconia ceramic processe...

2015
Natravee Chantranikul Prarom Salimee

PURPOSE The aim of this study was to evaluate the biaxial flexural strength (BFS) of one zirconia-based ceramic used with various veneering ceramics. MATERIALS AND METHODS Zirconia core material (Katana) and five veneering ceramics (Cerabien ZR; CZR, Lava Ceram; LV, Cercon Ceram Kiss; CC, IPS e.max Ceram; EM and VITA VM9; VT) were selected. Using the powder/liquid layering technique, bilayere...

Ardavan Etemadi, Fatemeh Gorjizadeh, Mohammad Hashem Hosseini, Pedram Baghaeian,

Background and Aim: Application of zirconia ceramics has increased. Since the commonly used surface treatment for porcelain, i.e. acid etching is not efficient for zirconia surfaces, evaluation of other surface treatment methods for zirconia is important. The aim of this study was to compare the shear bond strength (SBS) of metal brackets to zirconia treated with different powers of Er:YAG lase...

Journal: :Journal of lasers in medical sciences 2014
Shahin Kasraei Mohammad Atefat Maryam Beheshti Nassimeh Safavi Maryam Mojtahedi Loghman Rezaei-Soufi

INTRODUCTION Since it is not possible to form an adequate micromechanical bond between resin cement and zirconia ceramics using common surface treatment techniques, laser pretreatment has been suggested for zirconia ceramic surfaces. The aim of this study was to evaluate the effect of Carbon Dioxide (CO2) Laser treatment on shear bond strength (SBS) of resin cement to zirconia ceramic. METHOD...

2014
Shahin Kasraei Loghman Rezaei-Soufi Bijan Heidari Fariborz Vafaee

OBJECTIVES It is difficult to achieve adhesion between resin cement and zirconia ceramics using routine surface preparation methods. The aim of this study was to evaluate the effects of CO2 and Er:YAG laser treatment on the bond strength of resin cement to zirconia ceramics. MATERIALS AND METHODS In this in-vitro study 45 zirconia disks (6 mm in diameter and 2 mm in thickness) were assigned t...

2017
Amreen Rupawala Smita I. Musani Pallavi Madanshetty Ramandeep Dugal Umang D. Shah Ektaa J. Sheth

PURPOSE The purpose of this in vitro research project was to evaluate and compare the wear behavior of human tooth enamel opposing monolithic zirconia and other different ceramic restorative materials and also to observe the tetragonal to monoclinic phase transformation in zirconia-based ceramics that may occur while simulating wear occurring at room temperature in a wet environment. MATERIAL...

2007
Haksung Moon Je-Hyeong Bahk Fred F. Lange

We dedicate this work to Wolfgang Pompe, a very good friend and a good friend of the Materials Faculty at UCSB where he and his wife, Gisela, shared their lives and fellowship. Three different zirconia–alumina laminates, AZ50, AZ80, and AZ95, were fabricated via tape-casting thick Zr(3Y)O2 layers, dip-coating the zirconia tapes in a slurry containing a mixture of zirconia and alumina, stacking ...

2008
V. G. Varanasi

Equilibrium calculations were used to optimize conditions for the chemical vapor deposition (CVD) of zirconia. The results showed zirconia formation would occur at high oxygen to zirconium atomic ratios (N4), low hydrogen to carbon ratios (b10), low pressures (b105 Pa) and high temperatures (N800 °C). Using these calculations as a guide, single-phase monoclinic zirconia coatings were deposited ...

2017
Mohammed M Gad Ahmad M Al-Thobity Suliman Y Shahin Badar T Alsaqer Aiman A Ali

BACKGROUND Despite drawbacks, cold-cured acrylic resin is still the most common material used in denture repair. Zirconia nanoparticles were among the reinforcements added to increase the strength of the resin. The effect on Candida due to the addition of zirconia nanoparticles to the resin has not been investigated. PURPOSE The aim of this study was to evaluate the effect of zirconia nanopar...

A. Ghassemi, A. Najafi, F. Babaki, M. Abdo Tabrizi, M. Ekrami,

  Objective: Zirconia cores have limited light transmittance and data are scarce on light transmission through zirconia cores with and without the veneering ceramic.   Methods: In this in vitro study, Disc-shaped specimens (11.5 mm in diameter and 0.4 (0.05) mm in thickness) were fabricated of three types of zirconia namely Mamut, Heany and ZirkonZahn (n=5). A disc-shaped specimen (11.5 mm in d...