نتایج جستجو برای: hydroxyapatite coating
تعداد نتایج: 46544 فیلتر نتایج به سال:
We carried out a histological study of a proximally hydroxyapatite (HA)-coated femoral component, retrieved after 9.5 years of good function. The HA coating had completely degraded. Bone was in direct contact with the titanium surface in all the areas which had been coated, with no interposing fibrous tissue. There were no signs of particles, third-body wear, adverse tissue reactions or osteoly...
A biologically active material enables implants to bond with bone, which could significantly extend the lifetime of the artificial implants or other medical reconstructive devices. The bioactive coating adhere to the surface of the implant, binds with both implants and bone, promotes formation of hydroxyapatite and lengthens the implant lifetime. Such implants are more durable and long lasting ...
INTRODUCTION With the increase in joint revision surgery after arthroplasty, defects of hydroxyapatite (HA)-coated prostheses have been observed increasingly often. These defects adversely affect the prosthetic stability in vivo. This study has analyzed the potential effect of the adhesive strength of HA coating on the stability of HA-coated prostheses in vivo after its implantation. MATERIAL...
A novel strategy for the preparation of Si-doped hydroxyapatite (Si-HA) coatings on H2O2-treated carbon/carbon composites (C/C) was developed. HA coating was prepared on C/C through chemical liquid vaporization deposition (CLVD)/hydrothermal treatment. HA coating was immersed in an H2SiO3 solution at an autoclave at 413 K for transformation into Si-HA coating. The effects of H2SiO3 mass content...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید