ZHIYUAN YANG YANJUN TANG JUNHUA ZHANG

ZHIYUAN YANG, YANJUN TANG , JUNHUA ZHANG Key Laboratory of Advanced Textile Materials and Manufacturing Technology, Ministry of Education, Zhejiang Sci-Tech University, Hangzhou, 310018, China State Key Lab of Pulp and Paper Engineering, South China University of Technology, Guangzhou, 510640, China Engineering Research Center for Eco-Dyeing & Finishing of Textiles, Ministry of Education, Zheji...

Journal: :Materials & Design 2022

In the effort to find a balance between mechanical properties of self-healing styrene-butadiene rubber (SBR) compounds, before and after macroscopic damage, study based on use devulcanised tire residue (dGTR) as reinforcement has been carried out. Two full factorial designs their analysis variance (ANOVA) were used overcome challenge relating multiple microstructural variables dGTR compounds in...

Journal: :Sustainability 2021

In order to study the mechanical properties and effect of a regenerant on cold recycled mixture with asphalt emulsions (CRMEs), moisture susceptibility, high-temperature performance, low-temperature dynamic durability CRMEs were analyzed evaluated by immersion splitting strength tests, freeze-thaw rutting semi-circle bending uniaxial compression modulus tests indirect tensile tests. Scanning el...

2007
L. Bao K. Todaka I. Yamaura K. Kemmochi

Rubber material generally behaves as an electrical insulator, but vapor-grown carbon fiber (VGCF) is known for its electrical conductivity. Thus, we compounded styrene-butadiene rubber and carbon nanofiber (VGCF), and studied the relationship between strain and the DC electrical resistivity of vulcanized rubber filled with carbon nanofiber. No change of hardness was observed in hardness tests. ...

2012
Atsushi Asano Shunsuke Hori Masashi Kitamura Chikako T Nakazawa Takuzo Kurotsu

We have investigated the influence of the high centrifugal pressure caused by fast magic-angle spinning (MAS) on the molecular motion of styrene–butadiene rubbers (SBR) filled with SiO2 (SBR/Si composite) though solid-state magic-angle spinning nuclear magnetic Resonance (1H MAS NMR) measurements. Because the 1H–1H dipolar interaction of elastomers is weak compared with that of glassy polymers,...