In this work, two different laterites (iron contents of 13.07 and 49.34 wt%, respectively, for lateritic clay, LAC, iron-rich laterite, LAI) were selected calcined at 600 °C. The obtained laterites, namely LAI600 LAC600, separately mixed with an alkaline solution (silicate modulus 1.35) or acidic (phosphoric acid pH ≤ 2) the synthesis inorganic polymer products. fabricated products cured 20 °C ...