Journal: :British Dental Journal 2004

The aim of this study was to synthesis of glass ionomer-silk fiber composite and to evaluate the effect of adding natural degummed silk fiber on the mechanical properties of glass ionomer cement (GIC). For this purpose, natural degummed silk fibers with 1 mm in length and 13-16 µm in diameter were added to the ceramic component of a commercial glass ionomer cement in 1, 3 and 5 wt. %. Compressi...

ششمانی, مهسان, قلیچ خانی, زهرا, لطفیان, ملیحه,

Background and purpose: Deep fissures of occlusal surface in recently erupted first permanent molars are prone to accumulation of bacterial plaque. Sealing these fissures by appropriate flowing materials, as pit and fissure sealants, is a conservative way to prevent caries. The purpose of this study was to compare retention of flowable composite resin by resin modified glass ionomer sealant in ...

2013
Meenal Nitin Gulve Nitin Dilip Gulve

BACKGROUND Scuba diving is one of the fastest growing sports in the world. The objective of this study was to evaluate the effect of pressure variations to which divers are exposed on the pull out strength of glass fiber post luted with different cements. MATERIALS AND METHODS In this in vitro study, 120 extracted, single-rooted lower premolars were endodontically treated. They were randomly ...

Journal: :Journal of dentistry 1996
A Jokstad I A Mjör

OBJECTIVE The aim of the present clinical longitudinal study was to observe, over 10 years, the prognosis of abutment teeth restored with fixed prostheses retained by glass ionomer luting cements and one conventional zinc phosphate cement. METHODS Three dentists prepared 135 abutment teeth in 61 patients to retain 81 fixed prostheses. The prostheses were retained by two glass ionomer luting c...

Journal: :World Journal Of Advanced Research and Reviews 2022

Aim: To determine the rate of use dental materials in areas surgery, prosthodontics, periodontics, pediatric dentistry and orthodontics Dentistry Faculty University Cuenca, Ecuador. Materials methods: We analyzed 43 clinic weight these was obtained by a precision electronic scale to number doses, price per serving usage fee. Results: The glass ionomer for light-cured restoration powder presenta...

Journal: :The Journal of Nihon University School of Dentistry 1997
O Bala M Uçtaşli H Can E Türköz M Can

Fluoride release from six light-activated restorative materials, including two resinmodified glass-ionomers, two composites, and two compomers, was evaluated and compared with one conventional acid-based glass-ionomer cement. The amount and rate of release varied among the tested materials. Both resin-modified glass-ionomers and the conventional acid-base glass-ionomer cements released more flu...

2008
Elizabeta Gjorgievska John W. Nicholson Snezana Iljovska Ian J. Slipper

OBJECTIVE The aim of this study was to investigate the adaptation of different types of restorations towards deciduous and young permanent teeth. MATERIAL AND METHODS Class V cavities were prepared in deciduous and young permanent teeth and filled with different materials (a conventional glass-ionomer, a resin-modified glass-ionomer, a poly-acid-modified composite resin and a conventional com...

Abbas Makarem Amir Reza Motamedi Behjat-Al-Molook Ajami Masoumeh Ebrahimi Taraneh Movahhed

Introduction: In restorative dentistry, selecting the proper material is an important factor for clinical success. The objective of this study was clinical evaluation of survival time of three tooth color materials in primary anterior teeth. Methods: In this interventional clinical trial study, 94 deciduous anterior teeth (36 teeth in boys, 58 teeth in girls) belonging to 3-5 year old children ...

Journal: :Pediatric dentistry 1991
L Seppä H Forss

Seventy-one caries-free human occlusal fissures were used for this study. Twenty-two fissures were sealed with a glass ionomer sealant (Fuji Ionomer Type III--G-C Dental Industrial Corp., Tokyo, Japan), 24 were widened with a diamond bur and sealed with the glass ionomer sealant, and 25 were left unsealed. After one week, the sealants were removed as completely as possible with a probe. All fis...