copper–silver bimetallic strips were produced by cold roll welding process and were treated by diffusion annealing in the temperature range 250–800 ?c. the interface bonding strength was determined by bending and peeling tests, resistance, conductivity and micro hardness profiles were determined and microstructure in the interface region was observed by optical microscope. electrical resistance...
Eucalyptus regnans was subjected to thermal treatment. The samples were placed in superheated vapors at 120, 130, 140, 150, 160, 170, 180, 190, and 200 °C at ambient pressure to determine the effect of heat treatment on the physical-mechanical properties of Eucalyptus regnans. The results showed that heat treatment played an important role in the impact toughness, nail-holding ability, surface ...
Polymer blends composites were prepared according to the formula [84%LLDPE:15%((100-X)%PP:X%PVP):1%B.P] with weight ratios selected for X values (0,4,8,12,16 %), as strips by double screw extruder and use press process the strips to prepare the samples according ASTM specification, the mechanical properties were studied for all theprepared samples which are (tensile, flexural, compression, impa...
We present an X-ray fast-timing and spectral analysis of the type II bursts and the persistent emission (PE) of the Rapid Burster observed with the EXOSAT Medium-Energy Instrument. The Hardness-Intensity and Color-Color Diagrams of the Rapid Burster are somewhat different from those of the majority of other low-mass X-ray binaries, which fall into two distinct groups, “atoll” and “Z” sources. T...
High-strength low-carbon ferritic steels attaining a maximum yield strength of 1600 MPa by combined Cu and NiAl precipitationstrengthening were developed. The yield strength of the alloys increases monotonically with the total concentration of the principal alloying elements i.e. Mn, Cu, Ni and Al. At 12.40 at.%, a 1600 MPa yield strength is achieved after solution treatment at 950 C followed b...
BACKGROUND This study aimed to evaluate the flexural strength and microhardness of three different anterior composites after 10 000 thermocycles. MATERIAL AND METHODS The mechanical properties of a nano-fill composite (Filtek Ultimate Universal Restorative (FUR) (Enamel)), a nano-hybrid composite (Clearfil Majesty ES2 (ES2) (Enamel)), and a micro-hybrid composite (G Aenial Anterior (GAA)) wer...
Aiming at developing a dental titanium alloy with better mechanical properties and machinability than unalloyed titanium, a series of Ti-Nb alloys with Nb concentrations up to 30% was made. They were cast into magnesia-based molds using a dental casting machine and the mechanical properties and grindability of the castings were examined. The hardness of the alloys with Nb concentrations of 5% a...