Parametric Optimization of TIG Welding on Stainless Steel (202) & Mild Steel by using Taguchi Method
The main objective of industries reveal with manufacturing better quality product at low cost and increase productivity. TIG welding is most vital and common operation use for joining of two similar or dissimilar parts with heating the material or applying the pressure by using the filler material for increasing productivity with less time and cost constrain. The TIG welding parameters are the ...
In the present study, the microstructure and mechanical properties of the dissimilar joint of Inconel 625 (IN-625) superalloy to austenitic stainless steel AISI316L (SS-316L) via AWS-BNi3 interface layer and transient liquid phase (TLP) bonding process were evaluated and necessary conditions for creating an efficient joint were determined. TLP bonding was performed in temperature and time range...
The aerospace, automotive and marine industries have witnessed a rapid increase of using adhesive bonded joints due to their advantages in joining dissimilar and/or new engineering materials. Joint strength is the key property evaluating capability joint. In this paper, developments black-box grey-box machine learning (ML) models are presented allow accurate predictions failure load single lap ...
In this study, commercially pure titanium and aluminum alloy 5083 in connection rotational speed of 1120 rpm and a feed rate of 50 mm per minute for butt welding by friction stir welding has been successfully completed. Micro-structure, hardness and tensile test was conducted on the connection. Welding area is a composite of aluminum and titanium particles that the particles plays an important ...
Residual stresses induced by the welding processes may, in some cases, result significant warping and distortions that can endanger integrity of welded structures. This document reports an investigation process to make a dissimilar T-joint through advanced Finite Element (FE) modelling dedicated laboratory test. The consisted two plates materials, AISI304 S275JR steels, both having thickness 5 ...
To reduce costs and improve high-temperature performance in Advanced Ultra Super Critical (AUSC) boilers, it is necessary to weld austenitic steel Inconel alloy. In this study, the autogenous tungsten inert gas (TIG) welding process was used join Alloy 617 an AISI 304H plate of thickness 5 mm. Microstructural analysis showed that microstructure formation uneven along weldments, with columnar ce...