In this research, the wear behavior of commercial grades of WC-10wt%Co (H10F), WC-40vol%Co and WC-40vol%FeAl-B composites with different amounts of boron from zero to 1000 ppm has been investigated by the pin on disk test  method at high temperature. The wear tests were done under load of 40 N, a distance of 100 m and at ambient temperature, 200 ̊C and 300 ̊C. Wear surfaces were examine...

2013
Xuelin Lei Liang Wang Bin Shen Fanghong Sun Zhiming Zhang

Thin boron doped diamond (BDD) film is deposited from trimethyl borate/acetone/hydrogen mixture on Co-cemented tungsten carbide (WC-Co) micro drills by using the hot filament chemical vapor deposition (HFCVD) technique. The boron peak on Raman spectrum confirms the boron incorporation in diamond film. This film is used as an interlayer for subsequent CVD of micro-crystalline diamond (MCD) film....