2003
Raymond A. Pearson Albert F. Yee

An epoxy based on the diglycidyl ether of bisphenol A (DGEBA) has been modified with poly(phenylene oxide) (PPO) and cured with piperidine. A two-phase alloy resulted, in which the DGEBA epoxy was the continuous phase. Several PPO loadings were investigated. The tensile yield strengths of these PPO-modified epoxies were found to be independent of PPO content. In contrast, the fracture toughness...

2016
Wei-Cheng Chu Wei-Sheng Lin Shiao-Wei Kuo

In this study, we used diglycidyl ether bisphenol A (DGEBA) as a matrix, the ABA block copolymer poly(ethylene oxide-b-propylene oxide-b-ethylene oxide) (Pluronic F127) as an additive, and diphenyl diaminosulfone (DDS) as a curing agent to prepare flexible epoxy resins through reaction-induced microphase separation (RIMPS). Fourier transform infrared spectroscopy confirmed the existence of hydr...

2017
Xavier Ramis

A kinetic model for thiol–epoxy crosslinking initiated by tertiary amines has been proposed. The kinetic model is based on mechanistic considerations and it features the effect of the initiator, hydroxyl content, and thiol–epoxy ratios. The results of the kinetic model have been compared with data from the curing of off-stoichiometric formulations of diglycidyl ether of bisphenol A (DGEBA) cros...

2010
LAURA MURESAN SZILVESZTER GÁSPÁR GRAZIELLA TURDEAN IONEL CATALIN POPESCU

In our quest for a simple and fast method to detect glucose in wines, a redox polymer (RP)-based amperometric biosensor was developed. The biosensor consists of glucose oxidase and horseradish peroxidase (as recognition tandem), an Os-based RP (as electron transfer mediator), poly(ethylene glycol) diglycidyl ether (as cross-linking agent), and a graphite electrode (as transducer). Each building...

Journal: :Contact dermatitis 2016
Susanne Darr-Foit Johannes Geier Peter Elsner Sibylle Schliemann

A 63-year-old painter and varnisher presented with a 4-year history of work-related contact dermatitis affecting the dorsal surfaces of his hands, forearms, and face. He reported itching, burning and oozing when he occupationally handled epoxy resin systems. Patch testing was performed by the use of small Finn Chambers® on Scanpor® tape (SmartPractice Europe, Reinbek, Germany) with the baseline...

2013
Cai Jiang Jianwei Zhang Shaofeng Lin Dazhi Jiang

Molecular dynamic (MD) simulations were carried out to predict the thermo-mechanical properties of the cured epoxy network composed of diglycidyl ether bisphenol A (DGEBA) epoxy resin and tetrahydrophthalic anhydride (THPA) curing agent and their single-walled carbon nanotubes (SWCNT) reinforced the epoxy matrix composites. Different characters such as the density of the materials and mean squa...

2005
Preeti Jain V. Choudhary

The paper deals with the curing behaviour of diglycidyl ether of bisphenol-A (DGEBA) using three novel multifunctional aromatic amines having phosphine oxide and amide-acid linkages. The amines were prepared by reacting tris(3-aminophenyl)phosphine oxide (TAP) with 1,2,4,5-benzenetetracarboxylic acid anhydride (P)/4,4-(hexafluoroisopropylidene)diphthalic acid anhydride (F)/3,3,4,4-benzophenonet...

2004
R. A. PEARSON A. F. YEE

The role of matrix ductility on the toughenability and toughening mechanism of elastomermodified, diglycidyl ether of bisphenol A (DGEBA)-based epoxies is investigated. Matrix ductility is varied by using epoxide resins of varying epoxide monomer molecular weights. These epoxide resins are cured using 4,4' diaminodiphenyl sulphone (DDS) and, in some cases, modified with 10vol % carboxyl-termina...

Journal: :Food technology and biotechnology 2016
Gábor Csiffáry Péter Fűtő Nóra Adányi Attila Kiss

A novel biosensor for l-ascorbic acid determination in different beverages was elaborated. The ascorbate oxidase enzyme (AAO) from Cucurbita sp., EC 1.10.3.3, was immobilized on a screen-printed carbon electrode with poly(ethylene glycol) (400) diglycidyl ether (PEGDGE) as a crosslinking agent. The standards and samples were measured first with a blank electrode. An inert protein, bovine serum ...

2014
Mònica Mir Roberto Lugo Islam Bogachan Tahirbegi Josep Samitier

Poly(vinylchloride) (PVC) is the most common polymer matrix used in the fabrication of ion-selective electrodes (ISEs). However, the surfaces of PVC-based sensors have been reported to show membrane instability. In an attempt to overcome this limitation, here we developed two alternative methods for the preparation of highly stable and robust ion-selective sensors. These platforms are based on ...