Abstract The aim of this contribution is to present a comprehensive approach study the extent hydrogen entry into hot-dip-galvanized DP1000 steel, which exposed corrosive conditions. For purpose, Z100 coating was immersed in 5% sodium chloride solution at room temperature. distribution and spots increased were detected with scanning Kelvin probe (SKP) force microscopy (SKPFM). Effects inserted ...