Journal: :Corrosion Science 2023

Slow strain rate tests on hydrogen-containing specimens of PH13–8Mo maraging stainless steel showed H-assisted subcritical quasi-cleavage cracking, accelerating material failure. Fractographic analysis revealed that is composed flat brittle areas and rougher areas. Electron backscatter diffraction (EBSD) was performed a secondary subcritically grown crack. High resolution EBSD significant cryst...

Journal: :Journal of the Society of Materials Science, Japan 1998

Mehrabi Sharifabad, H., Hajisafari, M. ,

In this research, two different filler metals, ERNiCrMo-3 and ER309L, were used for developing different microstructure, austenite (γ) and austenite and ferrite (γ+δ) in the weld metal and fatigue properties of welded samples were evaluated in the air and sea water environments. Microstructural studies indicated a good agreement between predicted microstructures via schiffler diagram and metall...

Mehrabi Sharifabad, H., Hajisafari, M. ,

In this research, two different filler metals, ERNiCrMo-3 and ER309L, were used for developing different microstructure, austenite (γ) and austenite and ferrite (γ+δ) in the weld metal and fatigue properties of welded samples were evaluated in the air and sea water environments. Microstructural studies indicated a good agreement between predicted microstructures via schiffler diagram and metall...

Journal: :Journal of the Society of Materials Science, Japan 1986