The electrochemical and corrosion behaviour of Al-6061, Al-4.5%Cu and Al-7.5%Cu alloys were studied in 0.50 M KSCN solution at 25 C. Open-circuit potential, Tafel polarization and ICP-AES measurements were used to study the uniform corrosion process on the surfaces of the tested alloys. Cyclic polarization measurements were employed for pitting corrosion studies. Obtained results were compared ...
The influence of alloying additions on strengthening of high pressure torsion (HPT) processed alloys was investigated using commercially pure Al (Al-1050 alloy) and five Al-(1-3)Mg-(0-4)Cu alloys (in wt%). Microhardness was measured on cross sections. For Al-1050 the microhardness reaches a peak at an effective strain of about 3 and subsequently decreases. The microhardness of Al-Mg-Cu alloys i...
In this investigation ‚the fracture toughness of A356 containing15%SiC composite was studied. Al/SiC composites have been considered because of their mechanical and erosion properties .Low fracture toughness in Al/SiC as compared with Aluminium alloys is one of its disadvantage. In this study at first A356 alloy was melted in a smelting electrical furnace then poured into the mould. A356-15% Si...
In view of large interest in the improve of Al/Al alloy based Metal matrix Composite and high-temperature ceramics on the base of silicon carbide, a comprehensive review of the data on structure, properties and the known methods of processing of silicon carbide seems timely. The most striking feature of silicon carbide is its polytypism, i.e. formation of a great number of structural changes wi...
In the last decades, the class of Ti-rich TiAl-based intermetallic materials has replaced many contemporary alloys till 900 °C. Due to higher oxidation resistance, 20% lower density and higher (about 150 °C more) operating temperature possibility of Al-rich TiAl alloys over Ti-rich side, phases from the Al-rich region of this alloy system are considered to be highly potential candidates for hig...
in this study, the elemental powders of aluminum and copper were initially subjected to mechanical alloying using an attrition ball mill under argon atmosphere to produce an al-4.5 wt% cu powder alloy. the wc nanoparticles were then added to the powder alloy and milled in a planetary ball mill to explore the role of the wc nanoparticles on the mechanical properties of the fabricated composite p...
in this research a cu-zn-al alloy is produced by melting the raw materials in an electric resistance furnace and then pouring it into a steel mould. the optimum way to achieve the final analysis in the hypo-eutectoid range is determined and the influence of the alloying element, ti on the grain size and the shape memory properties of the samples are investigated. solution treatment (done at 850...