José María Parmigiani-Izquierdo María Eugenia Cabaña-Muñoz José Joaquín Merino Arturo Sánchez-Pérez

BACKGROUND One of the disadvantages of the zirconia implants is the lack of elasticity, which is increased with the use of ceramic or zirconia crowns. The consequences that could result from this lack of elasticity have led to the search for new materials with improved mechanical properties. CASE PRESENTATION A patient who is a 45-year-old woman, non-smoker and has no medical record of intere...

Journal: :journal of dentistry, tehran university of medical sciences 0
hossein bagheri tabassom hooshmand farzaneh aghajani

objectives: this study aimed to evaluate the effect of different ceramic surface treatments after machining grinding on the biaxial flexural strength (bfs) of machinable dental ceramics with different crystalline phases. materials and methods: disk-shape specimens (10mm in diameter and 1.3mm in thickness) of machinable ceramic cores (two silica-based and one zirconia-based ceramics) were prepar...

Journal: :Quintessence international 2011
Tonino Traini Marzia Pettinicchio Giovanna Murmura Giuseppe Varvara Nicola Di Lullo Bruna Sinjari Sergio Caputi

This article describes the high esthetic value of a single-tooth implant immediately placed in the anterior region using a flapless approach and a custom-made zirconia-ceramic abutment and crown. The case reported illustrates the practical procedure involved in developing natural esthetics with a custom-made zirconia-ceramic prosthesis and abutment. The technique is relatively simple, can be us...

2012
Satheesh B. Haralur Ali Hassan Al-Faifi

Proper, intelligent use of materials and technology should be utilized for the benefit of the patient. This case report presents a patient with a badly broken premolar tooth demanding high esthetic all-ceramic restoration. Following multiple procedure tooth was restored with zirconia all ceramic restoration. Multiple procedures to save a tooth are a really worthy, in the interest of patients. U...

2017
Uwe Scheithauer Steven Weingarten Robert Johne Eric Schwarzer Johannes Abel Hans-Jürgen Richter Tassilo Moritz Alexander Michaelis

In our study, we investigated the additive manufacturing (AM) of ceramic-based functionally graded materials (FGM) by the direct AM technology thermoplastic 3D printing (T3DP). Zirconia components with varying microstructures were additively manufactured by using thermoplastic suspensions with different contents of pore-forming agents (PFA), which were co-sintered defect-free. Different materia...

Journal: :The Journal of bone and joint surgery. British volume 2004
G Maccauro C Piconi W Burger L Pilloni E De Santis F Muratori I D Learmonth

We studied factors contributing to the initiation of fracture and failure of a zirconia ceramic femoral head. The materials retrieved during a revision total hip replacement were submitted to either visual, stereomicroscopic and scanning electron microscopy (SEM) or SEM and energy-dispersive X-ray analysis. X-ray diffraction was performed in order to investigate the extent of tetragonal to mono...

Abdollah Javan Rashid Ahmad Ghahremanloo Mohsen Movahedzadeh

Introduction: Marginal fit is a key factor for long term clinical success through any dental restorations. Poor marginal adaptation causes cement dissolution. This can lead to dental caries, gingival irritation, periodontal diseases, and finally treatment failure. The aim of this study was measurement and comparison of marginal gap quantities in metal ceramic and all ceramic dental restorations...

Journal: :avicenna journal of dental research 0
z. khamverdi associate professor, dept. of operative dentistry, dental research center, dental faculty, hamadan university of medical sciences, iranسازمان اصلی تایید شده: دانشگاه علوم پزشکی همدان (hamadan university of medical sciences) z. moshiri assistant professor; dep t . of prosthodontics, dental faculty , zanjan university of medical scienceسازمان اصلی تایید شده: دانشگاه علوم پزشکی زنجان (zanjan university of medical sciences)

the interest of dental research in metal-free restorations has been rising in the last 20 years following the introduction of innovative all-ceramic materials in the daily practice. in particular, high-strength ceramics and related cad/cam techniques have widely increased the clinical indications of metal-free restorations, showing more favorable mechanical characteristics compared to the early...

Journal: :Journal of dentistry 2015
Hossein Bagheri Tabassom Hooshmand Farzaneh Aghajani

OBJECTIVES This study aimed to evaluate the effect of different ceramic surface treatments after machining grinding on the biaxial flexural strength (BFS) of machinable dental ceramics with different crystalline phases. MATERIALS AND METHODS Disk-shape specimens (10mm in diameter and 1.3mm in thickness) of machinable ceramic cores (two silica-based and one zirconia-based ceramics) were prepar...

2016
Jing Li Xiaobei Wang Yuanhua Lin Xuliang Deng Ming Li Cewen Nan

Zirconia ceramics with porous structure have been prepared by solid-state reaction using yttria-stabilized zirconia and stearic acid powders. Analysis of its microstructure and phase composition revealed that a pure zirconia phase can be obtained. Our results indicated that its porosity and pore size as well as the mechanical characteristics can be tuned by changing the content of stearic acid ...