Harold Vernon first introduced acrylic polymers as denture base materials in 1937. A survey showed that 33% of denture repairs were to restore debonded teeth.1 Factors that affect the bonding of acrylic resin teeth to the denture base are dewaxing procedures, residual wax on ridge laps of teeth,2 and careless application separating media like sodium alginate to the teeth, leading to contaminati...
SAPO-11 is synthesized from silicoaluminophosphate in the presence of di-n-propylamine as a template. The results show that sample obtained has good crystallinity, 396m2/g BET surface area, and 0.35 cm3/g pore volume. hydroisomerization activity (0.25)Pt (1)Zr (0.5)W/SAPO-11 catalyst was determined using n-decane base oil. All experiments were achieved at fixed bed plug flow reactor temperature...